Flat Lap Technique
I have several disks 6-18 inches and a 24" lap . I would like to start using the succession of grinding disks to make these smooth and attach a 1"x7" inch dowel with waterproof duct tape to the back. I have checked locally and no one provides coldworking classes and because of commitments I cannot take off to Houston or where ever to take proper classes at this time. Could someone please share the best way to grind glass disks on a flat lap please?
Thank you Much!
Shereen
Thank you Much!
Shereen
Last edited by S.TImmerman on Fri Sep 14, 2012 4:42 am, edited 1 time in total.
Re: Flat Lap Technique
What happened with the dowel method?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
S.TImmerman
- Posts: 235
- Joined: Wed Nov 25, 2009 9:23 am
- Location: San Diego ,Ca
Re: Flat Lap Technique
Ah, someone else is a night owl ehMorganica wrote:What happened with the dowel method?
I so wish someone in southern calif taught coldworking as I just got my wet belt sander too. Bullseye has a short video on it which I'm thankful for!
-
David Jenkins
- Posts: 174
- Joined: Wed Apr 29, 2009 10:35 pm
- Location: Cypress, Texas
Re: Flat Lap Technique
Some questions/comments:
1. Your disks are 6-8" in diameter, and the lap has a 24" diameter wheel? If that's correct, I would think you'd have to be really, really careful of not letting your piece extend over the edge of the disk, or you'll risk getting grooves in the piece where it laps over. But I may be misinterpreting your post.
2. Are you polishing a glass disk? I have found that to be a difficult exercise - esp. in achieving a single-plane surface. Just the slightest variation in pressure on the dowel you're using will cause (or at least it has for me) a "faceting" of the surface you're trying to grind. YMMV, though.
3. I've followed instructions I've found elsewhere here (they may have been lost when the archives disappeared) as far using a broom handle piece as a handle. I make a piece that extends past the edges of the glass 3"-4" and just tape the bejabbers out of it using the good waterproof duct tape I got from HIS Glassworks. Works like a champ.
4. Do your disks have a hole in the center (for laps that feed water through a center hole)? I got one of those by accident, and even though it's essentially a flat disk, I've had problems with that center hole leaving marks on the glass if I move the piece back and forth over the hole. I'm guessing it's operator error, but until I perfect my technique, I avoid using that disk.
HTH
1. Your disks are 6-8" in diameter, and the lap has a 24" diameter wheel? If that's correct, I would think you'd have to be really, really careful of not letting your piece extend over the edge of the disk, or you'll risk getting grooves in the piece where it laps over. But I may be misinterpreting your post.
2. Are you polishing a glass disk? I have found that to be a difficult exercise - esp. in achieving a single-plane surface. Just the slightest variation in pressure on the dowel you're using will cause (or at least it has for me) a "faceting" of the surface you're trying to grind. YMMV, though.
3. I've followed instructions I've found elsewhere here (they may have been lost when the archives disappeared) as far using a broom handle piece as a handle. I make a piece that extends past the edges of the glass 3"-4" and just tape the bejabbers out of it using the good waterproof duct tape I got from HIS Glassworks. Works like a champ.
4. Do your disks have a hole in the center (for laps that feed water through a center hole)? I got one of those by accident, and even though it's essentially a flat disk, I've had problems with that center hole leaving marks on the glass if I move the piece back and forth over the hole. I'm guessing it's operator error, but until I perfect my technique, I avoid using that disk.
HTH
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Glass at Harbor Gates
Cypress, TX
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Flat Lap Technique
We use lg suction cups to hold the glass on our 24" flat lap..... Not sure what you are trying to do...
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
S.TImmerman
- Posts: 235
- Joined: Wed Nov 25, 2009 9:23 am
- Location: San Diego ,Ca
Re: Flat Lap Technique
I have rod disks that have hundreds of cut rods and disks that are round pot melts that range from 6-13". I remeasured the disks today. They are not very smooth and I want to perfect them before I slump them Into bowls. The flat lap grinder has 24 flat disks in several grades.
Laura, where do you buy the suction cups? May I have the link to ones you bought?
Yes,the disks have a hole but the water system comes up the side and I can position it wherever I want. This is the same lap that his glassworks sell but I bought it from grindglass.com
Thank you for any help
Shereen
Laura, where do you buy the suction cups? May I have the link to ones you bought?
Yes,the disks have a hole but the water system comes up the side and I can position it wherever I want. This is the same lap that his glassworks sell but I bought it from grindglass.com
Thank you for any help
Shereen
-
David Jenkins
- Posts: 174
- Joined: Wed Apr 29, 2009 10:35 pm
- Location: Cypress, Texas
Re: Flat Lap Technique
Sorry - I misinterpreted the disk measurement you cited - I thought you meant the abrasive disk was 6" in diameter, and you were talking about the glass disk. Right?
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Glass at Harbor Gates
Cypress, TX
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Flat Lap Technique
Suction cups can be great but........ it is possible to leave suction cup ring marks on the glass that show up on the finished piece. 
Re: Flat Lap Technique
CRL has the suction cups.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Flat Lap Technique
Something like these
http://sell.lulusoso.com/selling-leads/ ... e-etc.html
I have never had them leave a mark on the glass.
http://sell.lulusoso.com/selling-leads/ ... e-etc.html
I have never had them leave a mark on the glass.
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Flat Lap Technique
I guess Laurie that you haven't fired enough clear glass so as to experience the marking potential of suckers.
You've been lucky in other words.
The marks are 'invisible' until the glass is fired and pretty much cannot be removed once on the glass.
At least I've never figured out a surefire removal method other than not using suckers in the first place.
They can be seen by blowing warm breath onto cold glass.
In the old archives there was much discussion about this.
You've been lucky in other words.
The marks are 'invisible' until the glass is fired and pretty much cannot be removed once on the glass.
At least I've never figured out a surefire removal method other than not using suckers in the first place.
They can be seen by blowing warm breath onto cold glass.
In the old archives there was much discussion about this.
Re: Flat Lap Technique
Yup, been there, done that. Good cleaning required before firing.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Flat Lap Technique
I have seen
that..... All i do is take very fine steel wool and glass cleaner using some elbow grease and i do not have that problem. Lucky? I'll take it!
that..... All i do is take very fine steel wool and glass cleaner using some elbow grease and i do not have that problem. Lucky? I'll take it!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Re: Flat Lap Technique
I've used the suction cups and had them slip off during lapping, so be careful. If the glass isn't fused totally flat and your attention wavers a bit, you can jostle the cup enough to let in some air, destroying the vacuum and creating a lovely shrapnel effect as the glass flies across the room.
The piece needs to be clean for duct tape (and it's usually pretty clean straight out of the kiln, since oils and things have burned off). And you need a lot of duct tape, applied in multiple directions.
The piece needs to be clean for duct tape (and it's usually pretty clean straight out of the kiln, since oils and things have burned off). And you need a lot of duct tape, applied in multiple directions.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
S.TImmerman
- Posts: 235
- Joined: Wed Nov 25, 2009 9:23 am
- Location: San Diego ,Ca
Re: Flat Lap Technique
David Jenkins wrote:Sorry - I misinterpreted the disk measurement you cited - I thought you meant the abrasive disk was 6" in diameter, and you were talking about the glass disk. Right?
David, absolutely no problem!! I'm so greatful for all the experience of artists here . Perhaps it was me that didn't use the correct lingo. 8" Glass disks. =: about 1000 1/4 inch rods stacked up and fused into a "glass disks". (what is the proper lingo?)
-
S.TImmerman
- Posts: 235
- Joined: Wed Nov 25, 2009 9:23 am
- Location: San Diego ,Ca
Re: Flat Lap Technique
[quote="Laurie Spray"]Something like these
http://sell.lulusoso.com/selling-leads/ ... e-etc.html
I have never had them leave a mark on the glass.[/quote
Thank you Laura , btw I love all the items I've bought from you!
Morginia , thank you for the caution, I think ill get one that shows when it's losing suction so I can use the emergency break on the flat lap
I'll really clean them well with steel wool too
John at grindglass.com is the one that makes the flat laps for hisglassworks and is very nice to work with.
http://sell.lulusoso.com/selling-leads/ ... e-etc.html
I have never had them leave a mark on the glass.[/quote
Thank you Laura , btw I love all the items I've bought from you!
Morginia , thank you for the caution, I think ill get one that shows when it's losing suction so I can use the emergency break on the flat lap
I'll really clean them well with steel wool too
John at grindglass.com is the one that makes the flat laps for hisglassworks and is very nice to work with.
Re: Flat Lap Technique
. . . (what is the proper lingo?)
Blank.
Blank.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Flat Lap Technique
I do not use duct tape..... And i do use a sucktion cup that shows if it even starts to lose suction. I would not try to use one unless the bottom is totally flat.......i should have said that!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Flat Lap Technique
This is the technique that Els Vanden Ende was working on at Pilchuck in 2010; she did some really beautiful work that's now traveling in Bullseye's Act 2 The Glass Track show.S.TImmerman wrote: 8" Glass disks. =: about 1000 1/4 inch rods stacked up and fused into a "glass disks". (what is the proper lingo?)
http://www.bullseyeglass.com/kilnformin ... a-377.html
-
S.TImmerman
- Posts: 235
- Joined: Wed Nov 25, 2009 9:23 am
- Location: San Diego ,Ca
Re: Flat Lap Technique
This is the technique that Els Vanden Ende was working on at Pilchuck in 2010; she did some really beautiful work that's now traveling in Bullseye's Act 2 The Glass Track show.
http://www.bullseyeglass.com/kilnformin ... a-377.html[/quote]
Very nice work, thanks for sharing it, her name suggests she's Dutch, German maybe.. I'm Dutch
I want to eventually do designs with different colored rods. My New Paragon Caladra kiln quit after the 16th firing and I bought it for Vitrograph to pull canes - i had not set up yet and this happened. it is less than 3 months old
that gold colored wire is supposed to be attached to that white ceramic piece.
http://www.bullseyeglass.com/kilnformin ... a-377.html[/quote]
Very nice work, thanks for sharing it, her name suggests she's Dutch, German maybe.. I'm Dutch
I want to eventually do designs with different colored rods. My New Paragon Caladra kiln quit after the 16th firing and I bought it for Vitrograph to pull canes - i had not set up yet and this happened. it is less than 3 months old