Loctite Durabond 530CL- reviews?

Post by Bonnie Rubinstein »

Anyone have experience with Loctite Durabond 530CL?


Thanks!
Bonnie Rubinstein
Bonnie Rubinstein
Posts: 239
Joined: Sun May 04, 2003 9:04 pm
Location: River Falls, WI

Re: Loctite Durabond 530CL- reviews?

Post by Bonnie Rubinstein »

Just found out that product name was dropped- it is now Loctite E-30CL.
Bonnie Rubinstein
Tony Smith
Posts: 1037
Joined: Sun Mar 09, 2003 5:59 pm
Location: Massachusetts, USA
Contact:

Re: Loctite Durabond 530CL- reviews?

Post by Tony Smith »

I've used it. It's a strong epoxy. It's water clear. It requires a special applicator that costs more than the glue. It's not super thin, so it's hard to hide the bondline.