Alternative method of breaking glass

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Alexis Dinno
Posts: 57
Joined: Sun Dec 13, 2009 9:35 pm

Alternative method of breaking glass

Post by Alexis Dinno »

I caught wind of a few videos like this, where a small piece of ceramic thrown with not much force shatters the side-windows of an automobile.

http://www.youtube.com/watch?v=Vyw60MMC ... re=related

Can anyone help me understand the physics? When I break tempered glass, I generally need to tap it on edge with something hard, but I have literally hammered the flat face with no visible effect, so this video is surprising.
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Alternative method of breaking glass

Post by Brad Walker »

When you strike the flat surface of tempered glass with a hammer, the force of the blow is spread out across a broader area so that it doesn't shatter. If the hammer blow is at an angle or if the hammer head is very small or pointed, rather than flat, you can break tempered glass.

With a spark plug or similar small item, all of the force of the throw is directed to one small spot, rather than spread out. That's what causes the window to break. Porcelain is really hard and if a broken piece of spark plug is used you have very small pointed edges which make it easier to break the window.

As an aside, windshields (windscreens) are usually made of laminated glass (two layers with a plastic film between), while car windows are usually made of tempered glass. Using tempered glass allows a trapped occupant to break the glass from the inside. You can even buy hammers with a hardened steel point for the purpose of breaking the glass in an emergency. http://www.lifehammer.com/
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Alternative method of breaking glass

Post by Bert Weiss »

To simplify what Brad said
Tempered glass:
baseball : bounce Sharp point : shatter

The edge is more vulnerable than the surface. A hammer blow works fine on the edge. Another tool that will shatter the surface is an automatic center punch. This is a steel point in a spring loaded device. http://www.harborfreight.com/spring-loa ... h-621.html
Image
Last edited by Bert Weiss on Thu Sep 27, 2012 12:16 pm, edited 1 time in total.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Alexis Dinno
Posts: 57
Joined: Sun Dec 13, 2009 9:35 pm

Re: Alternative method of breaking glass

Post by Alexis Dinno »

I certainly knew where to ask this question. :D
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Alternative method of breaking glass

Post by The Hobbyist »

That spring loaded center punch is sold in Florida as an emergency escape tool if you should happen to drive your car into one of the many canals. It happens fairly often.

Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg