Using clear prismatic glass and powders

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Katie M
Posts: 8
Joined: Sat Mar 08, 2008 8:28 pm

Using clear prismatic glass and powders

Post by Katie M »

I would like to use a piece of Bullseye Clear Prismatic glass and then sift different colors of transparent powders into the channels of the glass to create a linear pattern. I've not done this before so I am unclear as to whether I should cap it with a layer of Crystal Clear or put the Prismatic glass with powders on top of a base layer of clear and fire it that way. Any advice?
Live life ..... you can sleep when you're dead!
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Using clear prismatic glass and powders

Post by Brad Walker »

Don't cap. Put the textured glass on a base piece of regular clear glass and then sift powder on top of the textured glass. Fire to a full fuse.
Katie M
Posts: 8
Joined: Sat Mar 08, 2008 8:28 pm

Re: Using clear prismatic glass and powders

Post by Katie M »

Thanks very much. Really appreciate the help this forum provides!