I would like to use a piece of Bullseye Clear Prismatic glass and then sift different colors of transparent powders into the channels of the glass to create a linear pattern. I've not done this before so I am unclear as to whether I should cap it with a layer of Crystal Clear or put the Prismatic glass with powders on top of a base layer of clear and fire it that way. Any advice?
Live life ..... you can sleep when you're dead!
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Using clear prismatic glass and powders
Don't cap. Put the textured glass on a base piece of regular clear glass and then sift powder on top of the textured glass. Fire to a full fuse.
Re: Using clear prismatic glass and powders
Thanks very much. Really appreciate the help this forum provides!