Fused Glass Drawer Pulls

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
David Jenkins
Posts: 174
Joined: Wed Apr 29, 2009 10:35 pm
Location: Cypress, Texas

Fused Glass Drawer Pulls

Post by David Jenkins »

Saw some very nice fused glass drawer pulls at a builders hardware supply store today. Anybody know where I can find ready-made findings for such items? I.e., flat metal strips or small squares (to which fused glass would be glued) with attached female threaded standoffs/posts.

Thanks.
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Fused Glass Drawer Pulls

Post by Brock »

Tennessee Tom on this board has some really nice ones, reasonably priced.
I think I paid around $50.00 for 21 a few years ago.
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Fused Glass Drawer Pulls

Post by bob proulx »

Brock wrote:Tennessee Tom on this board has some really nice ones, reasonably priced.
I think I paid around $50.00 for 21 a few years ago.
Brock, how do you find Tennesse Tom, I did a search and nothing came up.
Bob
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Fused Glass Drawer Pulls

Post by AndyT »

Slumpy's has pulls and knobs.
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Fused Glass Drawer Pulls

Post by Morganica »

I have a bunch from Confusion Art that work very well and are easy to use, with well-done specs and instructions so you know what you're getting. (Disclosure: Donna and Ed are friends of mine, but they really do make a high-quality product)

http://confusionartstudio.com/diy_hardw ... der_online
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: Fused Glass Drawer Pulls

Post by Brock »

Maybe Tennessee Tom is no longer a member. Morganica's supplier looks good.
Faye Malench
Posts: 46
Joined: Sun Jan 02, 2005 9:03 pm
Location: Illinois
Contact:

Re: Fused Glass Drawer Pulls

Post by Faye Malench »

Tom Furman also sent me a few knob samples to test along with advice on best adhesives. I have not followed-up on making them yet but have a more local source to me near St. Louis. Take a look at these - http://www.dlawlesshardware.com/knob-making-bases.html. They wrote telling me many items are back-ordered but will be available mid-October
David Jenkins
Posts: 174
Joined: Wed Apr 29, 2009 10:35 pm
Location: Cypress, Texas

Re: Fused Glass Drawer Pulls

Post by David Jenkins »

Thanks, all. I clearly wasn't diligent enough in my searching - the darn things are all over the place.
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
katesaunders
Posts: 21
Joined: Mon Mar 17, 2003 1:37 pm
Location: oregon coast

Re: Fused Glass Drawer Pulls

Post by katesaunders »

Go to one of the big building supply stores, like Home Depot, and check out drawer pulls. I've gotten some decent pulls and used them with my glass. Much cheaper
then buying pulls made specifically to make glass drawer pulls from. Recently I found some drawer handles at Ikea which would be perfect for larger handles.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: Fused Glass Drawer Pulls

Post by jim simmons »

The folks at Aquila glass school has a very nice collection of both knobs and pulls.goto
http://www.hotknobs.com/
I can vouch for them because I help teach a beginning fusing class there.
Jim
Tom Fuhrman
Posts: 187
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: Fused Glass Drawer Pulls

Post by Tom Fuhrman »

bob proulx wrote:
Brock wrote:Tennessee Tom on this board has some really nice ones, reasonably priced.
I think I paid around $50.00 for 21 a few years ago.
Brock, how do you find Tennesse Tom, I did a search and nothing came up.
Bob
well after a lengthy go around and Brad's help I am finally able to post on here again. He told me I was the only one on the board that had an e-mail address that would not recognize the soft ware running on the board.
I still have some solid brass pulls in polished brass and unfinished brass that I would make someone a tremendous deal on. I also figured out a way to redrill them and add a set screw to make them into door knobs, etc. anyone interested send me an e-mail and I'll send some pics of them.
Tenn. Tom
aka www.fuhrmanglass.com