Hi,
I have a Paragon Janus Ovation 10 Multipurpose Kiln that fires from the lid and two upper side elements (for glass) and from the sides only (for ceramics) at the flip of a switch. So far I have used it only for glass. I am considering selling my ceramic kiln and firing clay projects in the Ovation as well as my glass projects. Does the off-gassing from firing clay cause any contamination of subsequent glass projects fired in the same kiln? Has anyone fired both in your kiln?
Thanks!
Ginny
Ceramic Firing Contaminants?
Moderators: Brad Walker, Tony Smith
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Ceramic Firing Contaminants?
do both. no worries. rosanna
artist, owner of wanchese art studio, marine finisher
Re: Ceramic Firing Contaminants?
Thanks Rosanna! 