Has anyone used George's Rigidizer? It is a blue-green liquid. I coated 1/8 inch fiber with it but noticed the back was still white. Should I coat the back as well? There was no instructions for pre-firing it.
Thanks,
Dave
George's Rigidizer
Moderators: Brad Walker, Tony Smith
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: George's Rigidizer
i would coat both sides. Fire to whatever temp you are going to use it at kiln wash and use .rosannat
artist, owner of wanchese art studio, marine finisher
Re: George's Rigidizer
Thanks Rosanna