Blenko
Moderator: Brad Walker
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Blenko
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Blenko
Out of curiousity I emailed a question to Blenko the other day. They got back with me quickly, and again quickly to a follow-up question I asked. I'll paraphrase from their email.
Blenko still sells sheet glass.
They have sheet glass sample sets for $20.00 per set.
They will send of a few samples if you are just interested in just a few colors.
When we wish to know which colors Blenko has on hand for immediate shipment, we may inquire via email or call.
The rep I corresponded with provided her email and individual contact information, I shouldn't post that here. You can reach them like I did initially at:
info@blenkoglass.com
Sheet Glass Price List
Blenko Antique Sheet Glass
Regular Blenko colors $15.40/ sq.ft.
Reds, Oranges, Yellows $ 17.50/ sq.ft.
*maximum size 18”x 25” (untrimmed)
Historic Wood Mold Antique Sheet
*Clear Only
For Restoration Installation $ 17.50/ sq.ft.
*maximum size 18”x 25” (untrimmed)
*Custom cut – Call for Quote
* Sheet Glass sample sets $ 20.00
Packing cost
$ 40.00 per Antique Carton
(Approximately 30-35 sheets per case)
Freight charges calculated on day of shipment
Freight is FOB Shipping Point, Milton, WV
All freight shipments will be collect or on customers freight account
Prices subject to change without warning please call to verify pricing before placing your order.
9 Bill Blenko Drive
P.O. Box 67
Milton, WV 25541
Tel: 304-743-9081
Toll free: 877-425-3656
Fax: 304-743-0547
Blenko still sells sheet glass.
They have sheet glass sample sets for $20.00 per set.
They will send of a few samples if you are just interested in just a few colors.
When we wish to know which colors Blenko has on hand for immediate shipment, we may inquire via email or call.
The rep I corresponded with provided her email and individual contact information, I shouldn't post that here. You can reach them like I did initially at:
info@blenkoglass.com
Sheet Glass Price List
Blenko Antique Sheet Glass
Regular Blenko colors $15.40/ sq.ft.
Reds, Oranges, Yellows $ 17.50/ sq.ft.
*maximum size 18”x 25” (untrimmed)
Historic Wood Mold Antique Sheet
*Clear Only
For Restoration Installation $ 17.50/ sq.ft.
*maximum size 18”x 25” (untrimmed)
*Custom cut – Call for Quote
* Sheet Glass sample sets $ 20.00
Packing cost
$ 40.00 per Antique Carton
(Approximately 30-35 sheets per case)
Freight charges calculated on day of shipment
Freight is FOB Shipping Point, Milton, WV
All freight shipments will be collect or on customers freight account
Prices subject to change without warning please call to verify pricing before placing your order.
9 Bill Blenko Drive
P.O. Box 67
Milton, WV 25541
Tel: 304-743-9081
Toll free: 877-425-3656
Fax: 304-743-0547