Kiln Cooling

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
tgotch
Posts: 36
Joined: Mon Nov 14, 2011 11:04 pm

Kiln Cooling

Post by tgotch »

I have been playing around with my new kiln and slumping bottles I had a question on kiln cool down.

Is there a temperature at which you open the door to help expedite cooling? I have some people say to "crack" the door at ~400 degrees, and ok to open at ~200.

What do you do? Is there any other alternatives to expedite cool down?
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Kiln Cooling

Post by Kevin Midgley »

Do not rush when firing bottles. Keep kiln closed until near room temp.
They are uneven thickness.
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Kiln Cooling

Post by Stephen Richard »

Ditto to what Kevin says. The uneven thickness means any quick change of temperature in the 100-200ºC range will allow the thinner parts to cool quickly enough to induce thermal shock.
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
rosanna gusler
Posts: 730
Joined: Mon Mar 10, 2003 2:22 pm
Location: wanchese north carolina
Contact:

Re: Kiln Cooling

Post by rosanna gusler »

yep. just for s&g take a pair of calipers and measure the thick part of a slumped bottle. it can be suprisingly thick. rosanna
artist, owner of wanchese art studio, marine finisher
Morganica
Posts: 1079
Joined: Mon May 19, 2003 6:19 pm
Location: Portland, OR
Contact:

Re: Kiln Cooling

Post by Morganica »

A fused bottle is also a bit more prone to stress than a solid chunk of glass would be at that thickness. With a bottle the collapsed sides come together but may not completely fuse together in spots, especially if there are bubbles. Wherever the glass separates, that joint is an increased opportunity for stress, which actually argues for increasing the time, not decreasing it.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com

"I wrote, therefore I was." (me)
Post Reply