Hi all,,I have cut float glass into hearts using a tutorial I saw on youtube by Dee...that is one half to heart then the other half...I am wanting to fuse this BEFORE I sprinkle enamel on..have used magic tape to hold 2 pieces together,,,will this work?? will it fuse or pull apart?..have thought about putting a piece of float glass down the middle, put didnt think to use the same piece as I was cutting.. so this is just a crap shoot...just wondering if anyone has done the same..Thanks
bothofushk
fusing float glass side by side
Moderators: Brad Walker, Tony Smith
-
bothofushk
- Posts: 42
- Joined: Sat Jan 22, 2005 3:10 pm
- Location: East Texas
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: fusing float glass side by side
if it is just 3mm float no it will not work. if it is 6mm float it will still probably not work. . i would lap one over the pther and then fuse. rosanna
artist, owner of wanchese art studio, marine finisher
-
bothofushk
- Posts: 42
- Joined: Sat Jan 22, 2005 3:10 pm
- Location: East Texas
Re: fusing float glass side by side
Thanks, Rosanna, will try that...no harm no foul