OPAQUE Bullseye WHITE?

Post by Havi »

Hello eveybody,
I want to cover some stupidity I made.
I have a very dark top layer of glass. Behind, fused to it, I have broken sheet of tekta - I was wrongly assuming that the break will not be seen, because of the darkness of the glass. Unfortunately this does not happen.

My solution is to block the light coming from behind, by adding another layer.
I am sure it will work with black glass, but I prefer not to use black, rather white. Is there any hope that there is an absolutely opaque white that will block the light from behind as good as black? or is it just a wishful thinking?


Many thanks in advance,


Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: OPAQUE Bullseye WHITE?

Post by Brad Walker »

Bullseye makes an Opaque White, 0013-30. It is very dense, not as dense as black, of course, but it doesn't let much (if any) light through.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: OPAQUE Bullseye WHITE?

Post by Havi »

Thanks, Brad -
do you think that white CAN actually prevent seeing the break?
The dark color I have is BE 1108 - a beautiful color in itself.




Thanks,
Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: OPAQUE Bullseye WHITE?

Post by Brad Walker »

Havi wrote:Thanks, Brad -
do you think that white CAN actually prevent seeing the break?
The dark color I have is BE 1108 - a beautiful color in itself.
I wouldn't know without testing a small piece. Perhaps someone else on the board has tried it to see.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: OPAQUE Bullseye WHITE?

Post by Havi »

Thanks,
I think I won't take more chances. Take black and
Be safe

thanks,
Good night,



Havi
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: OPAQUE Bullseye WHITE?

Post by Warren Weiss »

Havi,
Hold the piece of white behind it and see if any light comes through. Whites usually become more opaique after fireing.
Warren
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: OPAQUE Bullseye WHITE?

Post by Havi »

Thanks, Warren
To be honest, what worries me about the white is , that it will make the top layer less dark , and this in itself will make the break more visible.
I want very much to use white, but as I said I am afraid that it will miss the aim for which it is put there.

Another thought that came to. Me is, that perhaps I could block the transparency with additional opaque color that will maybe add another dimension to the piece - like maybe another blue, or similar, just thinking aloud. I think I have to post a photo of this, to clarify myself.


Thanks anyway,

Havi