Pens that don't burn off.

Post by vblue »

I need to do some testing of a process and would like to mark on my pieces the measurement used. (That way I don't have to keep looking for my notes in my messy workroom.)

What can I use to mark on my glass with that won't burn off?

Thanks,
Vernelle
S.TImmerman
Posts: 235
Joined: Wed Nov 25, 2009 9:23 am
Location: San Diego ,Ca

Re: Pens that don't burn off.

Post by S.TImmerman »

"pilot" pens in gold and silver have worked for me in the past. You can also thin glass enamel paint and use a nib.
St
aeshep
Posts: 17
Joined: Mon Mar 21, 2011 1:56 pm

Re: Pens that don't burn off.

Post by aeshep »

Dykem brand. Bullseye website shows white that they use for marking hot glass. Here's the link: http://shop.bullseyeglass.com/catalogse ... k&x=7&y=10
haleybach
Posts: 75
Joined: Tue Sep 04, 2012 1:59 pm
Location: Austin TX

Re: Pens that don't burn off.

Post by haleybach »

Pilot gold and silver pens, gold can turn light blue at higher temps (1450? Maybe).

The ones listed on Amazon as "Pilot Gold and Silver Permanent Marker, Extra Fine Point, Set of 2 Markers (41400)
by Pilot"

I have found them at Wallgreen's (in Texas) among other places, they are fairly common.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Pens that don't burn off.

Post by Kevin Midgley »

Bic whiteout pens. Not necessarily compatible within a fused piece.

Check for xylene contents in these marker type pens. It burns at low temperatures. :-k