Blood!!
Moderators: Brad Walker, Tony Smith
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Blood!!
So i am building a very compicated and time consuming strip piece in a stainless steel ring......I just dropped a large drop of blood from a cut onto the already set up strips. I hate to take it all apart.....dang......do you think it will just burn off at full fuse?
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Blood!!
No, blood contains iron etc. and it has left marks on my glass before. 
Re: Blood!!
Just say you signed in blood.
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Blood!!
Dang! I figured as much! Thanks
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Blood!!
well, you could always bleed on it more and call it a design element. rosanna. ow that was bad i will stop n ow.
artist, owner of wanchese art studio, marine finisher
Re: Blood!!
Well, they say that artists ARE supposed to put themselves into their work... 
I think it depends on what kind of glass you drip on, aren't some glasses more reactive to iron contamination than others? OTOH, doin' some figgerin'... there's about 0.026 milligrams of iron in the average drop of human blood. Not a lot. I'd clean off the top surface and in the cracks as much as possible, but I'm not sure I'd worry about whatever seeped down in between the strips.
(For all the times I've dripped blood onto glass while assembling I'm kinda surprised I haven't seen much contamination, especially since I'm full of irony.)
I think it depends on what kind of glass you drip on, aren't some glasses more reactive to iron contamination than others? OTOH, doin' some figgerin'... there's about 0.026 milligrams of iron in the average drop of human blood. Not a lot. I'd clean off the top surface and in the cracks as much as possible, but I'm not sure I'd worry about whatever seeped down in between the strips.
(For all the times I've dripped blood onto glass while assembling I'm kinda surprised I haven't seen much contamination, especially since I'm full of irony.)
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Blood!!
Good one!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Blood!!
Peroxide zaps blood stains out of clothing; I wonder if you could drip a little in between the strips?
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Blood!!
GROAN,!!!!!!!!
Jim
Jim
Morganica wrote:.
(For all the times I've dripped blood onto glass while assembling I'm kinda surprised I haven't seen much contamination, especially since I'm full of irony.)