Has anyone used a Mezuzah mold or a seder plate mold? Any tips? Do you use fiber paper in the mezuzah mold or just kiln wash?
Can the mezuzah be slumped in the same load as a small plate that is also being slumped? Any guidances would be much appreciated.
Mezuzah mold?
Moderator: Tony Smith
Re: Mezuzah mold?
Hi. I don't have an answer for you but in the same vein of the conversation, I just, last night, slumped a mezzuzaha I made free form over a stack of fiber paper. Instead of the mezzuzahs slumping over the fiber paper, it somehow "arched up". So I will be following this thread closely to see what advice is given.
Thanks.
Rachel
Imaglassydiva@aol.com
Thanks.
Rachel
Imaglassydiva@aol.com
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Mezuzah mold?
Do you have a picture?
Jim
Jim
RachelM wrote:Hi. I don't have an answer for you but in the same vein of the conversation, I just, last night, slumped a mezzuzaha I made free form over a stack of fiber paper. Instead of the mezzuzahs slumping over the fiber paper, it somehow "arched up". So I will be following this thread closely to see what advice is given.
Thanks.
Rachel
Imaglassydiva@aol.com
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Mezuzah mold?
The size and weight of the glass determine how long it takes to slump. Chances are a mezzuzah will take longer than a bowl or seder plate. However, as long as you don't go too hot, I see no reason why the larger won't wait around for the smaller.Hannah Love wrote:Has anyone used a Mezuzah mold or a seder plate mold? Any tips? Do you use fiber paper in the mezuzah mold or just kiln wash?
Can the mezuzah be slumped in the same load as a small plate that is also being slumped? Any guidances would be much appreciated.
I make mezzuzot using silica fiber twisted rope. I dust it with alumina hydrate and then drape over it. It is all about how good you get at doing the shin. There are a myriad of ways to do it.
You can make a seder plate mold by cutting holes in a fiber board. Just cook until the cups form. With a drop style of mold, I would only do one thing at a time. If you are slumping in to a formed mold, it will be far more forgiving.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Mezuzah mold?
Thank you, Bert, for sharing how you form the mezzuzah. The mold I saw advertised is pretty expensive and it won't give me the "look" I am going after.