Post by katesaunders »

I just found out that Morton is no longer making those big white cutting boards, which I've been using for years. Although I've cut back a lot of my production work, I still
use that cutting system a lot. It's not unusual for me to cut up five or six sheets of glass a day--I need some way to easily set up sheets of glass to cut into rectangles, strips, squares, in exact duplication. I have a good circle cutter so it's only straight lines I need to cut. With Morton's I just adjust a metal bar and secure the glass and cut away. How do others do it? Thanks! Kate
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: new cutting system needed--no more Morton's!

Post by AndyT »

Morton is making an interlocking grid system. Two per pack so you'd need 2 packs to make a large grid surface. Creator's Stained Glass also makes a 4 pack and a 6 pack and works with all the Morton products.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: new cutting system needed--no more Morton's!

Post by Kevin Midgley »

Check out the grid light diffusers for fluorescent tube lights at your local building supply centre.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: new cutting system needed--no more Morton's!

Post by Laurie Spray »

tap plastics......they have large and larger boards that fit all the parts
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: new cutting system needed--no more Morton's!

Post by AndyT »

Kevin Midgley wrote:Check out the grid light diffusers for fluorescent tube lights at your local building supply centre.
You would need to mount that to some sort of base otherwise everytime you picked it up the glass shards that have fallen into the spaces would just end up on your workspace.
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: new cutting system needed--no more Morton's!

Post by AndyT »

Laurie Spray wrote:tap plastics......they have large and larger boards that fit all the parts
I couldn't find anything at Tap that even came close to the Morton boards.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: new cutting system needed--no more Morton's!

Post by jim simmons »

Tap in Tigard caries it in both white and silver.
1/2 inch spacing ans sheeets are 24 X 48 in stock
. 15230 SW Sequoia Pkwy. Tigard, OR 97224. Open: Mon-Fri 8:30 to 6, Sat 9 to 5. Phone: 503.620.4960 ...
Geeze, I sound like I work there.
Good luck Kate.
Jim

AndyT wrote:
Laurie Spray wrote:tap plastics......they have large and larger boards that fit all the parts
I couldn't find anything at Tap that even came close to the Morton boards.
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

Re: new cutting system needed--no more Morton's!

Post by jim simmons »

If all you want to do is to cut straight lines, Aquila glass school in Portland has a very good system.
Jim


[quote="katesaunders" It's not unusual for me to cut up five or six sheets of glass a day--I need some way to easily set up sheets of glass to cut into rectangles, strips, squares, in exact duplication.
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: new cutting system needed--no more Morton's!

Post by Valerie Adams »

AndyT wrote:
Laurie Spray wrote:tap plastics......they have large and larger boards that fit all the parts
I couldn't find anything at Tap that even came close to the Morton boards.
My (small) Tap has them in stock. I found this link (they're the Egg Crate version):
http://www.tapplastics.com/product_info ... ght_panels

I've also seen them at Lowes and Home Depot.
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: new cutting system needed--no more Morton's!

Post by AndyT »

Searched the entire site and couldn't find anything that looked like the Morton cutting surfaces.
jim simmons wrote:Tap in Tigard caries it in both white and silver.
1/2 inch spacing ans sheeets are 24 X 48 in stock
. 15230 SW Sequoia Pkwy. Tigard, OR 97224. Open: Mon-Fri 8:30 to 6, Sat 9 to 5. Phone: 503.620.4960 ...
Geeze, I sound like I work there.
Good luck Kate.
Jim

AndyT wrote:
Laurie Spray wrote:tap plastics......they have large and larger boards that fit all the parts
I couldn't find anything at Tap that even came close to the Morton boards.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: new cutting system needed--no more Morton's!

Post by Laurie Spray »

I kind of like the open back on the tap plastics board. Clean up is so easy. Just pick up the board and brush off the table into a trash can.
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
haleybach
Posts: 75
Joined: Tue Sep 04, 2012 1:59 pm
Location: Austin TX

Re: new cutting system needed--no more Morton's!

Post by haleybach »

Do these cut down for smaller sizes well? What do you cut them with?
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: new cutting system needed--no more Morton's!

Post by AndyT »

Valerie Adams wrote:
AndyT wrote:
Laurie Spray wrote:tap plastics......they have large and larger boards that fit all the parts
I couldn't find anything at Tap that even came close to the Morton boards.
My (small) Tap has them in stock. I found this link (they're the Egg Crate version):
http://www.tapplastics.com/product_info ... ght_panels

I've also seen them at Lowes and Home Depot.
Ah...light diffusers. Several choices at Lowes and Home Depot.
katesaunders
Posts: 21
Joined: Mon Mar 17, 2003 1:37 pm
Location: oregon coast

Re: new cutting system needed--no more Morton's!

Post by katesaunders »

I bought the smaller Morton cutting boards, which attach together. Haven't used them yet because now I see that I need to buy another 2 to make a big board. So I'm still not sure how well they'll work, but I will try Tap before I buy the other two Morton boards. And thanks Jim for all the information, next trip to Portland and I'll stop at Tap's. Thanks for all the feedback on this problem, since it did give me another gray hair or two. When I first started fusing glass I used to do all my cutting on the floor with a metal edge and I didn't want to do that ever again! Thanks again, Kate
Linda Gilpin
Posts: 12
Joined: Fri Oct 28, 2005 8:47 am
Location: Duncanville, TX

Re: new cutting system needed--no more Morton's!

Post by Linda Gilpin »

I'm also looking for a new cutting system. I'm thinking of one of those "wall mounted" cutters.(I've got a good saw for smaller pieces, but struggle with full sheets.) Best place to buy one? Any thoughts or advice on those?
Post Reply