I collect beach glass. Some of my pieces are large, ex., bottom of bottles. I use the pieces in jewelry and in mobiles. I am wondering if I can paint a beach scene on the beach glass and then fire the piece in my kiln according to the directions on the paint?
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Paints

Post by Bert Weiss »

LAF wrote:I collect beach glass. Some of my pieces are large, ex., bottom of bottles. I use the pieces in jewelry and in mobiles. I am wondering if I can paint a beach scene on the beach glass and then fire the piece in my kiln according to the directions on the paint?
yes
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Paints

Post by Brad Walker »

So long as you have a paint that's made to fire in the kiln. Look for glass enamels, such as Sunshine Enamels.

(Disclaimer: we sell Sunshine, so are biased toward them. www.warmglass.org)
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: Paints

Post by bob proulx »

Would you not lose the beach glass look at those temps. I sandblast glass ( system 96 ) and depending to what temp I go to I can bring the glass back to clear. Puebo, I think that's the name makes a glass paint that you can cure at 350 degrees. I have never put sea glass in a kiln so I could be wrong here
Bob
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Paints

Post by Brad Walker »

bob proulx wrote:Would you not lose the beach glass look at those temps. I sandblast glass ( system 96 ) and depending to what temp I go to I can bring the glass back to clear. Puebo, I think that's the name makes a glass paint that you can cure at 350 degrees. I have never put sea glass in a kiln so I could be wrong here
Bob
Depends on the paint you use and the temperature you fire to. Sunshine can mature around 1350F, which may be too high to retain the beach glass look. But there are other enamels that mature at lower temperatures, as well as traditional stained glass paints. And you're right, there is a paint that is oven cured -- Pebeo makes it -- that would work well. The only issue I can think of with the Pebeo paints is that they don't last as long as the kiln-fired enamels.
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Paints

Post by Judd »

Compatibility can also be an issue with true fired-on enamels. You'll need to do some test firing.
Stephen Richard
Posts: 302
Joined: Sun Jul 06, 2003 4:36 pm
Location: Glasgow, Scotland
Contact:

Re: Paints

Post by Stephen Richard »

Reusche glass stainers' enamels fire at 520ºC to 580ºC. Their colour is intense enough to require only a thin layer that is not affected by the type of glass (and does not affect the glass).
As much of the beach glass is bottle glass and so similar to float glass, these temperatures will not affect the surface of the glass much, if at all.
(2500 - what a chatterbox!)