Hello!
I have been able to reuse some plaster/silica open face molds for low temp fired pate de verre. If I fill these already fired molds with dry frit, is there any reason to vent my kiln?
Need to vent kiln if reusing a plaster/silica mold?
Moderator: Brad Walker
-
Yardic Glassworks
- Posts: 80
- Joined: Sat Mar 06, 2010 9:29 am
Re: Need to vent kiln if reusing a plaster/silica mold?
Nope, unless you are using some sort of glue or other material containing moisture.