Was working on a project using my Taurus Ring Saw and the blade broke. After changing the blade, a series of cuts that took a lot of pressure on the blade and about 5 minutes now takes less than a minute and very little pressure on the blade. Who Knew? Guess I should think about changing my grinder head.
Every once in a while I have to call myself out for being too cheap and foolish.
Every once in a while I have to call myself out for being too cheap and foolish.
Scott B
-
Nicole Hanna
- Posts: 27
- Joined: Wed Jul 27, 2005 10:17 am
- Location: SW Missouri
- Contact:
Re: Penny Wise and Pound Foolish
I do the same thing, but those blades are so darn expensive ya just hate to not use it till it finally screams and breaks on ya!
Nicole