I just finished the remaking of a piece that I made last month. The initial piece had BE013 which developed stress after a number of firings. This piece has had 8 firings without stress, and without any BE013. The first one became a giveaway, and 5lbs. of BE013 became a throwaway. Live and learn.
			
							
			
									
						
										
						- 
				JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Remake frit painting
Wow -- beautiful. I love the reflection in the water.
Dana W.
			
			
									
						
										
						Dana W.
Re: Remake frit painting
Just love it   You sure master this composition
  You sure master this composition
Thank you for sharing
Sophie
			
			
									
						
										
						 You sure master this composition
  You sure master this compositionThank you for sharing
Sophie

- 
				Jane Morgan
- Posts: 28
- Joined: Sat Sep 01, 2007 11:49 pm
- Location: Central Coast of California
- 
				Babette (Shawn)
- Posts: 103
- Joined: Fri Feb 05, 2010 4:11 pm
- Location: Chico California
- Contact:
Re: Remake frit painting
Nice piece David! I also dumped all of my  BE0013 powder.
			
			
									
						
							“Art washes away from the soul the dust of everyday life.” 
― Pablo Picasso
			
						― Pablo Picasso
Re: Remake frit painting
I was at Art Palm Beach last month...and believe I saw some of your work.  Captivating and sensuous use of light and shadow.  Very, very well done.
			
			
									
						
										
						- 
				jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Remake frit painting
lovely piece
			
			
									
						
							"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
			
						Re: Remake frit painting
Thanks for the comments, I appreciate it. It's validating to get encouragement from the glass community. Risa, my work was at Art Palm Beach last month with my gallery (unfortunately I wasn't there). They sold a large piece to someone they called a "major collector", whatever that means. It can't hurt.
			
			
									
						
										
						- 
				Zane
- Posts: 12
- Joined: Mon Mar 10, 2003 12:58 pm
- Location: moved to Illinois (not Chicago) in 2006 from Wisconsin
Re: Remake frit painting
Very lovely piece!
			
			
									
						
										
						- 
				glass-lady
- Posts: 18
- Joined: Sun Apr 25, 2004 2:43 pm
- Location: Wilmington, NC
- Contact:
Re: Remake frit painting
Fantastic.
			
			
									
						
										
						Re: Remake frit painting
Wow!  That is gorgeous!  That is what I'm aspiring to.   Ohhh....One day I hope...
  Ohhh....One day I hope...
			
			
									
						
							 Ohhh....One day I hope...
  Ohhh....One day I hope...Every artist was first an amateur.~ Ralph Waldo Emerson
			
						- 
				Delberta D
- Posts: 24
- Joined: Wed Mar 16, 2011 10:08 pm
Re: Remake frit painting
This is what I would love to learn to do. I have used Michael Dupilles technique but I want my picture to have NO bubbles....I did oil painting many years back and love these results in glass. Your piece is beautiful.
			
			
									
						
										
						Re: Remake frit painting
What did you use in place of BE013? That opaque white?david n wrote:I just finished the remaking of a piece that I made last month. The initial piece had BE013 which developed stress after a number of firings. This piece has had 8 firings without stress, and without any BE013. The first one became a giveaway, and 5lbs. of BE013 became a throwaway. Live and learn.

"C'est Moi (Its Me)"
- 
				jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Remake frit painting
Wonderful piece.  Anyone else looking to dump their 0013..you can dump it my way. 
			
			
									
						
							
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
			
						Re: Remake frit painting
Very nice indeed.
May I ask what are you using instead of BE0013?
I am curiuos, have you or anybody else incurred problems with BE0013 in other forms? like sheets, or big frit? [03]
Thanks,
Havi
			
			
									
						
							May I ask what are you using instead of BE0013?
I am curiuos, have you or anybody else incurred problems with BE0013 in other forms? like sheets, or big frit? [03]
Thanks,
Havi
Haviva Z 
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
			
						- - - - with a smile

"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
Re: Remake frit painting
I replaced the BE013 with BE113 (white opal) and it worked fine. I like the BE243 for snow, but it can't withstand the vitrograph temp. it turns partially clear. BTW I just returned from The Glass Weekend at Wheaton Arts in NJ today. My gallery sold this piece Sat. It was an amazing experience with demos and lectures from well-known glass artists (many collectors there too). It's held every other year. I would recommend it to anyone who loves glass.
			
			
									
						
										
						- 
				oatkaglass
- Posts: 5
- Joined: Fri Feb 29, 2008 8:27 pm
Re: Remake frit painting
Beautiful work David....haven't heard from you in awhile but it looks like you have been busy.
For anyone looking to take a class in this technique, Miriam di Fiore teaches her technique in her studio in Italy and also at various studios in the US. We are hoping to have her back teaching in our studio, Oatka School of Glass, in November 2014......
			
			
									
						
										
						For anyone looking to take a class in this technique, Miriam di Fiore teaches her technique in her studio in Italy and also at various studios in the US. We are hoping to have her back teaching in our studio, Oatka School of Glass, in November 2014......
- 
				Zane
- Posts: 12
- Joined: Mon Mar 10, 2003 12:58 pm
- Location: moved to Illinois (not Chicago) in 2006 from Wisconsin
Re: Remake frit painting
Gorgeous!
			
			
									
						
										
						- 
				Linda Gilpin
- Posts: 12
- Joined: Fri Oct 28, 2005 8:47 am
- Location: Duncanville, TX
Re: Remake frit painting
Beautiful work David!!  Have you used the new Warm White instead of the BE13?  Any problems, or would it dull it down a touch?  Thoughts?
			
			
									
						
										
						- 
				twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Remake frit painting
Oh so very beautiful!!!!!!!!!   Les
			
			
									
						
							Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
			
						website: http://www.twinvision.fusedglassartists.com