When I am using the cork belt with my belt sander, should it be wet or dry?
Thanks.
The other Jim
need cork belt info.
Moderator: Tony Smith
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: need cork belt info.
Wet. No cerium.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
S.TImmerman
- Posts: 235
- Joined: Wed Nov 25, 2009 9:23 am
- Location: San Diego ,Ca
Re: need cork belt info.
I have a 24" lap cerium pad
with c erium. Do I absolutly need to get a cork belt? on my =wet/wel
thank yiou
with c erium. Do I absolutly need to get a cork belt? on my =wet/wel
thank yiou
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: need cork belt info.
No. The cerium will do as good a job as the cork.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun