MR-97 mold release
Moderator: Brad Walker
MR-97 mold release
I'm using MR-97 Boron Nitride spray for my frit molds. The glass that was in contact with the mold has a satiny sheen rather than a glossy finish. The side not in contact with the mold is glossy. Am I just not getting all the mold release off? Or am I doing something wrong? How can I scrub it off? Thanks!
Every artist was first an amateur.~ Ralph Waldo Emerson
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: MR-97 mold release
Anything touching a mold, whether protected with BN, shelf paper or kiln wash, is going to have a different finish than the "air side".
Dana W.
Dana W.
Re: MR-97 mold release
Thanks JestersBaubles! I think I was either misinformed, or I misunderstood because I believe I was told that part of the benefit to using BN rather than kiln wash, was so it would have a nice glossy finish. I guess I'm scrubbing for nothing. I didn't mind the finish so much when I did flowers, but I did a dragonfly and I wanted the wings to be very translucent and they're not. I was kinda disappointed.
Every artist was first an amateur.~ Ralph Waldo Emerson
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: MR-97 mold release
Talk to Larry at colour deveere
He will give you the straight skinny
He will give you the straight skinny
Celene wrote:I'm using MR-97 Boron Nitride spray for my frit molds. The glass that was in contact with the mold has a satiny sheen rather than a glossy finish. The side not in contact with the mold is glossy. Am I just not getting all the mold release off? Or am I doing something wrong? How can I scrub it off? Thanks!
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: MR-97 mold release
If you want both sides to be glossy, you can either do a drop slump, blow glass, or torch work it. Contact with a mold dulls the finish, and adds texture. Partial contact with the mold is the worst, as you get some of each.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: MR-97 mold release
Thanks Bert! You've given me some good advice and things to think of!
Every artist was first an amateur.~ Ralph Waldo Emerson