Float glass base with 2" x 3" surface area UV adhesive strong connection...Any suggestions on separating?.. I tried soaking underwater for days with no effect. I'm wondering if heat will work?
Thanks, Don
Undo UV connection
Moderators: Brad Walker, Tony Smith
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Undo UV connection
"The Glassman"
-
Michele gh
- Posts: 71
- Joined: Tue Sep 21, 2004 11:10 pm
- Location: Massachusetts
- Contact:
Re: Undo UV connection
I have removed fused glass, which was attached to float with UV glue, with a slow firing up to 800°F.
Re: Undo UV connection
The adhesive we use breaks down at about 350.
I put it in a convection over, bring it up at about 100 degrees per hour, grab it with oven mitts and it usually comes apart pretty easily.
Then I clean it up with razor blade and rubbing alcohol.
Guy
I put it in a convection over, bring it up at about 100 degrees per hour, grab it with oven mitts and it usually comes apart pretty easily.
Then I clean it up with razor blade and rubbing alcohol.
Guy
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Undo UV connection
Try soaking in acetone. That will soften many adhesives.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Michele gh
- Posts: 71
- Joined: Tue Sep 21, 2004 11:10 pm
- Location: Massachusetts
- Contact:
Re: Undo UV connection
Although the bond between the two pieces of glass was broken somewhere between 300-400°F, the higher temperature made the residue easier to remove.
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: Undo UV connection
Thanks all for the input..I'll slowly heat it up as advised.
Don
Don
"The Glassman"
-
Rick Wilton
- Posts: 273
- Joined: Sat Oct 25, 2003 8:18 pm
- Location: Calgary, Canada
- Contact:
Re: Undo UV connection
Microwave,
Works like a charm, it heats the glue as it's the only organic material in there.
done it dozens of times.
Works like a charm, it heats the glue as it's the only organic material in there.
done it dozens of times.