How to check top loader for slump

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
JeffP
Posts: 25
Joined: Fri Feb 22, 2013 8:51 am
Location: Queensland, Australia

How to check top loader for slump

Post by JeffP »

Hi
I have a Paragon Fusion 14 which is a top loader, elements in lid, and peep hole on side.
Just put in my first attempt at a slump and realised I can't actually see to the bottom of the mold :oops: to see if it has slumped fully.
I assume that opening the lid to look is a bad thing, so how do I know when the slump is complete, other than let the schedule run and see?
Thanks
Jeff
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: How to check top loader for slump

Post by Brock »

Looking briefly at slumping temps is no problem.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: How to check top loader for slump

Post by Kevin Midgley »

protect your eyeballs etc.
JeffP
Posts: 25
Joined: Fri Feb 22, 2013 8:51 am
Location: Queensland, Australia

Re: How to check top loader for slump

Post by JeffP »

Brock wrote:Looking briefly at slumping temps is no problem.
Thanks Brock. I was concerned that it would remove too much heat, or worse crack the plate.
JeffP
Posts: 25
Joined: Fri Feb 22, 2013 8:51 am
Location: Queensland, Australia

Re: How to check top loader for slump

Post by JeffP »

Kevin Midgley wrote:protect your eyeballs etc.
I am wearing green kiln glasses, but I had someone say to me that even that isn't full protection and I should only look when absolutely necessary. What is your take on this? Do the glasses offer fully protection or only partial?
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: How to check top loader for slump

Post by Kevin Midgley »

I rarely look. Don't want cataracts.
Murphy's law says bleep drops on the glass from opening and closing lid during firing.
Check the suppliers above.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: How to check top loader for slump

Post by Laurie Spray »

You can open it enough to take a quick good look. Wear good long gloves and you will be fine (no longnhair, syn clothes). You just never want your glass to fall below 1100 is my rule.
Take your first look around 1200 if it is a shallow mold. Take notes so next time you will not have to open!
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: How to check top loader for slump

Post by Brock »

I think observing safety precautions is a good idea. However, I didn't know any better and looked in my kilns daily for over 20 years. I'm not recommending it, but sometimes dangers are exaggerated to ensure compliance.
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Re: How to check top loader for slump

Post by Brock »

JeffP wrote:
Brock wrote:Looking briefly at slumping temps is no problem.
Thanks Brock. I was concerned that it would remove too much heat, or worse crack the plate.
No, you'll be fine.
You can open, take a look and close and you'll only lose 50 degrees, or so.
Post Reply