pre-slump question?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
slats
Posts: 110
Joined: Thu Sep 04, 2003 9:19 pm

pre-slump question?

Post by slats »

I have a fused piece that I want to slump into a large square mold. The piece has pattern bars on the sides which spread at a bit in the fuse and now extends over the side os the mold by 1/8 of an inch. Should I cut this down, fire polish then slump? Will this 1/8 make a difference?
Brock
Posts: 1519
Joined: Mon Mar 10, 2003 1:32 pm
Location: Vancouver, B.C.

Post by Brock »

An 1/8" is probably okay. A 1/2" is not. Brock
My memory is so good, I can't remember the last time I forgot something . . .
Tim Swann
Posts: 83
Joined: Mon Mar 10, 2003 9:47 pm
Location: San Diego, CA

Post by Tim Swann »

I agree with Brock. 1/8â€
Post Reply