Arranging glass on shelf
Moderators: Brad Walker, Tony Smith
Arranging glass on shelf
Does anyone have any tricks on how to transfer complicated glass pattern to kiln shelf? I have it all arranged on a computer generated geometric paper pattern, but now getting it arranged on the shelf without the aid of the printed pattern is the problem. Take a photo maybe? Gotta be a better way. I guess I could put the paper on the kiln shelf and then slide the paper out. (sort of like the waiter pulling the table cloth) but that would cause some shifting.
jim
jim
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Arranging glass on shelf
Try printing it on thinfire
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
Re: Arranging glass on shelf
It's a CAD design. Can you run thinfire through a printer?
jim
jim
Re: Arranging glass on shelf
Probably depends on your printer's sensitivity. Try printing out a smaller design on an 8-1/2 X 11 piece and see if it jams or not.
Re: Arranging glass on shelf
Do you have a lighttbox? Maybe you can trace the pattern onto the shelf paper using your laser print out.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Arranging glass on shelf
We've had good luck printing on thinfire with our Laser printer.
If that doesn't work, you could also use an Artograph. It's a device that any art school or art student should be familiar with. Basically, it projects the drawing onto a surface, which could be the wall, the floor, or a kiln shelf. We have one, but we're in North Carolina. If there's an art school near you, you may be able to find someone that could lend you theirs.
If that doesn't work, you could also use an Artograph. It's a device that any art school or art student should be familiar with. Basically, it projects the drawing onto a surface, which could be the wall, the floor, or a kiln shelf. We have one, but we're in North Carolina. If there's an art school near you, you may be able to find someone that could lend you theirs.
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Arranging glass on shelf
pantograph ????
Re: Arranging glass on shelf
I'd be tempted to draw it on the shelf with Saral graphite wax-free transfer paper. Don't know how much that would visually contaminate though.
Re: Arranging glass on shelf
Thanks everyone. I let you know what worked.
jim
jim
Re: Arranging glass on shelf
I must be missing something here--why don't you just use plain old paper? It burns out completely between 500-600F (actually, remember Bradbury's Fahrenheit 451?). Unless the energy of combustion is powerful enough to move the glass (not likely, since you're going to have at least 6mm of glass weighting down all parts of the paper), it should be pretty straightforward.
I'd use thinner paper, the cheapest I could find because it's less likely to have clay coatings or other things that could leave a residue. There might be a fine ash underneath the finished glass, but unless the glass is moving it shouldn't trap the ash. Just set the paper on the shelf, arrange your glass, and go.
Whether you print on thinfire or regular paper, you will want to think about what you're printing WITH. Iron-rich laser toner is used in printing decals precisely because it leaves a mark on the glass. I'm not sure if any of the inkjet inks will leave a mark, never really tried it. I'd make a few tests first to get the processes and workflow down before spending time on the actual project.
I'd use thinner paper, the cheapest I could find because it's less likely to have clay coatings or other things that could leave a residue. There might be a fine ash underneath the finished glass, but unless the glass is moving it shouldn't trap the ash. Just set the paper on the shelf, arrange your glass, and go.
Whether you print on thinfire or regular paper, you will want to think about what you're printing WITH. Iron-rich laser toner is used in printing decals precisely because it leaves a mark on the glass. I'm not sure if any of the inkjet inks will leave a mark, never really tried it. I'd make a few tests first to get the processes and workflow down before spending time on the actual project.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Arranging glass on shelf
Get it on the shelf on top of the paper, dam the perimeter, and pull the paper out.
I have printed 1/32" 970 fiber paper in an inkjet printer. It worked fine. Thinfire should work too.
I have printed 1/32" 970 fiber paper in an inkjet printer. It worked fine. Thinfire should work too.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: Arranging glass on shelf
DO NOT print regular fiber paper in an inkjet or laser printer unless you just don't care about the printer, or you're willing to clean out the residue regularly. Modern printers are notoriously persnickety about paper crumbs, and regular fiber paper just isn't that tightly compressed. It's liable to shed. And unless the paper is polished it's going to be so absorbent that ink from an inkjet printer is likely to spread. That's not an issue for most prints, but if this is a high-tolerance CAD print the ink could bleed enough to make precision placement difficult.Bert Weiss wrote:Get it on the shelf on top of the paper, dam the perimeter, and pull the paper out.
I have printed 1/32" 970 fiber paper in an inkjet printer. It worked fine. Thinfire should work too.
Thinfire is polished and probably less of a problem..but if your printer puts paper through rollers that flip the paper upside down for printing, thinfire is also brittle enough to also cause some shedding/cracking problems.
Again, why not just use regular paper?
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Arranging glass on shelf
Hmm...burn the paper. The thought did cross my mind but it seemed too easy I guess. I'll do a test and let you know.
jim
jim
Re: Arranging glass on shelf
Test went fine. Used some standard white printer paper with printed 1/4" solid black lines. Fired to 1500 degrees x 30 minutes. Small amount of ash residue stuck to glass. It mostly scratched right off. Had to sandblast off a couple spots which could also have been kiln wash. Small price to pay for time saved arranging glass. No ink left on glass. Works for me.
Thanks again guys
Thanks again guys
-
bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Arranging glass on shelf
This is what I like about this board, you learn something new every time you visit.
Bob
Bob
Re: Arranging glass on shelf
If it's inkjet printer paper it may have a coating designed to trap and hold the ink. If the coating is clay or something inorganic, it's more likely to leave residue. The best paper is usually cheap newsprint, although it's also more absorptive so the ink won't be as precise.jjeakle wrote:Test went fine. Used some standard white printer paper with printed 1/4" solid black lines. Fired to 1500 degrees x 30 minutes. Small amount of ash residue stuck to glass. It mostly scratched right off. Had to sandblast off a couple spots which could also have been kiln wash. Small price to pay for time saved arranging glass. No ink left on glass. Works for me.
Thanks again guys
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
Re: Arranging glass on shelf
To test your inks
print on normal printing paper.
Lit the paper i the air.
Look thr script, if it is visible when the paper turns to ash, the ink will stau in the kiln, too.
print on normal printing paper.
Lit the paper i the air.
Look thr script, if it is visible when the paper turns to ash, the ink will stau in the kiln, too.