slumping glass into a glazed ceramic mold

Post by Peter Angel »

Hi all.

I remember reading a post on this board about how to apply kiln wash to a glazed ceramic mold (eg a platter or a bowl) and slumping glass into it.

I can't find the post.

Does anyone know how to get the kiln wash to stick well to the glazed ceramic?
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
bob proulx
Posts: 186
Joined: Tue Dec 29, 2009 7:13 pm
Location: Nahant Massachusetts
Contact:

Re: slumping glass into a glazed ceramic mold

Post by bob proulx »

I sandblast first then kiln wash, you have to scuff it up.
Bob
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: slumping glass into a glazed ceramic mold

Post by Valerie Adams »

I don't have a sandblaster so I use that mesh gritty sandpaper.
Karyn Cott
Posts: 13
Joined: Wed Sep 28, 2005 4:19 am
Location: Poulsbo, WA

Re: slumping glass into a glazed ceramic mold

Post by Karyn Cott »

I use Universal Mold Coat that Boyce Lundstrum developed. You add acrylic paint to the powder mixture and it lasts through several firings. No need to scuff the surface and it leaves the back of the piece very smooth. I love the product.
Karyn

"It is one of the blessings of old friends that you can afford to be stupid with them."
Ralph Waldo Emerson
Buttercup
Posts: 637
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: slumping glass into a glazed ceramic mold

Post by Buttercup »

Faye posted this previously:

Re: Porcelain Kitchenware for Slumping?
by Faye Malench » Thu Nov 22, 2012 12:22 am
A fast down and dirty method on glazed ceramic surfaces is to coat with spray adhesive, then dust on a layer of dry kiln wash. I use my small glass enamel/powder dispenser to make a smooth layer. The glue burns out but the powder stays in place. Have gotten multiple uses if the mold surface is not disturbed. Can't recommend it for a deep slump or one with detail, as the glass may drag the dry powder as it moves. Great for a shallow shape if you are in a hurry.

Faye, hope you don't mind my re-posting this? Jen
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: slumping glass into a glazed ceramic mold

Post by Peter Angel »

Valerie Adams wrote:I don't have a sandblaster so I use that mesh gritty sandpaper.
Valerie, what is mesh gritty sandpaper? Is it the same thing as course sandpaper?
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: slumping glass into a glazed ceramic mold

Post by Kevin Midgley »

Peter google 3m drywall sanding mesh.
Way better than sandpaper for sanding shelves.
Mike Griffin
Posts: 23
Joined: Mon Apr 01, 2013 10:04 pm
Location: Gelorup, Western Australia

Re: slumping glass into a glazed ceramic mold

Post by Mike Griffin »

I've bought a few glazed plates for slumping. They are often cheap, sometimes very cheap and occasionally you can pick up a plate that has a shape unlike anything that is available in slumping moulds or ceramic bisque. The most difficult task is drilling vent holes as the fully baked porcelain is hard. I do not prepare the glazed surface in any way either by roughening the surface or by spraying it with anything. I simply mix the kiln wash with water to a consistency of smooth un-thickened cream and taking a moistened Haik brush loaded with the 'cream' gently brush on one coat with parallel strokes. You can touch it up while it is wet but always in the one direction. Once it dries out any high spots can be lightly sand papered back. You should find the coating very durable so it should last for many slumpings.
Laurie Spray
Posts: 321
Joined: Sat Dec 17, 2005 10:32 pm
Location: SANTA CRUZ, CALIFORNIA
Contact:

Re: slumping glass into a glazed ceramic mold

Post by Laurie Spray »

If it is a shallow form such as a plate you do not need vent holes.......
Laurie Spray

New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Buttercup
Posts: 637
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: slumping glass into a glazed ceramic mold

Post by Buttercup »

[quote="Mike Griffin"]I've bought a few glazed plates for slumping. They are often cheap, sometimes very cheap and occasionally you can pick up a plate that has a shape unlike anything that is available in slumping moulds or ceramic bisque. The most difficult task is drilling vent holes as the fully baked porcelain is hard.

Mike, if you have access to sandblasting equipment you can mask, expose tiny circles and blast. The abrasive will eat through the glaze without the risk of shattering the plate. Jen
glass-lady
Posts: 18
Joined: Sun Apr 25, 2004 2:43 pm
Location: Wilmington, NC
Contact:

Re: slumping glass into a glazed ceramic mold

Post by glass-lady »

Absolutely love Lundstrom's Universal Mold Coat. Works like a dream. Can use glazed $1.50 dishes from Old Time Pottery. No need for holes if the slope is no higher than around 2 inches. This is wonderful, wonderful, wonderful stuff.