Hi alL
Can I re-use a pot for a pot-melt?
I understand that there will remain some glass on the pot after having fired it. Is it still possible to re-use the pot?
I plan to do my own clay pot, as I want to be million % sure it is clay and nothing else. Can it be re-used ?.
Any tips as to how to construct it? Bigger, squarish hole? etc.
Many thanks,
Havi
POT MELT, AGAIN
Moderators: Brad Walker, Tony Smith
POT MELT, AGAIN
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
-
David Jenkins
- Posts: 174
- Joined: Wed Apr 29, 2009 10:35 pm
- Location: Cypress, Texas
Re: POT MELT, AGAIN
Yes, you can re-use it. But I'd make sure that the colors/glasses you use on the nth use will work with the ones used in previous melts with that pot.
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Glass at Harbor Gates
Cypress, TX
Re: POT MELT, AGAIN
Thanks, Dave.
Havi
Havi
Haviva Z
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com
- - - - with a smile
"Speed comes from the Devil" - (an Arabic proverb)

http://www.havivaz.com