Hi
My weekend project is to figure out how to replicate a strip constructed project I completed at a class. The strips and windows are cut and I plan to put them together tomorrow. I did not take good enough notes on setting up the dams around the constructed project. I've searched the forum but do not see a clear description of how to set this up. Can someone either point me to a previous discussion on the forum or describe the process? I recall the dams get strips of fiber paper between the dams and the glass. I'd appreciate any comments. Thanks.
Susan
Dams & strip construction
Moderator: Tony Smith
-
Susanbuckler
- Posts: 68
- Joined: Tue Aug 18, 2009 10:31 pm
Dams & strip construction
Susan Buckler
Woodstock, NY
Woodstock, NY
Re: Dams & strip construction
I am jumping in with a second question for those answering.
If we use strips of fiber paper around the dams, do we still need to kiln wash the actual dams?
Susan - thanks for letting me tag along onto the thread!
Rachel
Imaglassydiva@aol.com
If we use strips of fiber paper around the dams, do we still need to kiln wash the actual dams?
Susan - thanks for letting me tag along onto the thread!
Rachel
Imaglassydiva@aol.com
Re: Dams & strip construction
One of the best tutorials I know of is Steve Immerman's at Clearwater Glass http://www.clearwaterglass.com/Tutorial ... ction.html. He is a master at strip construction, as you'll see from his site! Good luck.
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Dams & strip construction
Apply kilnwash to the dams. It's cheap insurance against a leak and it only needs to be done once. Use fiber paper that is shorter than the height of the glass strips and the edges will round over without needles.
Tony
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
Susanbuckler
- Posts: 68
- Joined: Tue Aug 18, 2009 10:31 pm
Re: Dams & strip construction
Thanks to all.
I also found a video on BE
https://www.bullseyeglass.com/education ... n-165.html
Steve Immerman's work is so precise....and beautiful.
Susan
I also found a video on BE
https://www.bullseyeglass.com/education ... n-165.html
Steve Immerman's work is so precise....and beautiful.
Susan
Susan Buckler
Woodstock, NY
Woodstock, NY
Re: Dams & strip construction
His stuff is just beautiful. I love the precision. I wish he would teach, but I guess he might be kind of busy with his day job.Susanbuckler wrote:Thanks to all.
I also found a video on BE
https://www.bullseyeglass.com/education ... n-165.html
Steve Immerman's work is so precise....and beautiful.
Susan