removing grease pencil from glass
Moderators: Brad Walker, Tony Smith
removing grease pencil from glass
how? acetone doesn't do it very well, neither does glass cleaner. Anyone? anyone?
"Every artist was first an amateur."
--Ralph Waldo Emerson
--Ralph Waldo Emerson
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: removing grease pencil from glass
whiting and scrubby pad and elbow grease? Bon Ami if you can still find it.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: removing grease pencil from glass
goo gone?
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: removing grease pencil from glass
Magic Erasers -- they work great on glass.
Dana W.
Dana W.
Re: removing grease pencil from glass
Usually I use a razor blade to scrape off most of it, then let the area soak in acetone, window cleaner, denatured alcohol, whatever's handy, and rub the rest of it right off.
It's a different matter if the glass has texture to it--grease pencil in roughened irid/dichro, or tight little nooks and crannies in a tack fuse is a real bear to remove.
It's a different matter if the glass has texture to it--grease pencil in roughened irid/dichro, or tight little nooks and crannies in a tack fuse is a real bear to remove.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery