My kids are here for a couple of days, and want to try an art project that starts by heating rocks in the oven to 350 degrees.
Do I need to fear them exploding when heated??
Any advice would be appreciated,
Thanks,
Loraine
JamesL
Posts: 29
Joined: Wed May 18, 2011 1:08 pm

Re: Urgent HELP needed

Post by JamesL »

Do a You-Tube search for "Exploding Rocks" and you will see some kids heating rocks over a camp fire. They do "pop" or "explode". I have read that some rocks that are heated aggressively will crack, shatter, etc. Weather that's from internal moisture or the kind of rocks they are, I'm not sure.
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Urgent HELP needed

Post by Brad Walker »

If a rock has moisture in it, it will explode when heated.

If a rock does not have moisture in it, it will not explode, but it might crack anyway.

Most rocks have moisture.

(Not sure why this was urgent, by the way. Urgent is when your kiln is exploding, not a couple of rocks. <grin>)
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Urgent HELP needed

Post by Valerie Adams »

Invert a stainless steel bowl over the rocks so if they break apart in your kiln, they'll be contained.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Urgent HELP needed

Post by Bert Weiss »

Sandstone is the most famous exploding rock. I have tried to fire granite, but that did not go well. It cracked.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Glass Fever
Posts: 29
Joined: Sat Aug 04, 2007 11:08 pm
Location: Chicago Suburbs
Contact:

Re: Urgent HELP needed

Post by Glass Fever »

She's asking about heating to 350F in an oven, not firing at high heat. I think you should be OK at 350. If I was going to do this I'd put them in the oven without preheating.
Brad Walker
Site Admin
Posts: 1537
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Urgent HELP needed

Post by Brad Walker »

Glass Fever wrote:She's asking about heating to 350F in an oven, not firing at high heat. I think you should be OK at 350.
Why? If the rocks have moisture in them, the water would turn to steam long before you reach 350.
lorwolff
Posts: 22
Joined: Sun Apr 19, 2009 5:37 pm
Location: Keyport and Seattle, Washington

Re: Urgent HELP needed

Post by lorwolff »

Thanks everyone, I apologize for saying 'Urgent'..., you're right, I don't want to cry wolf. (But when it comes to grandkids, I get crazy and over-zealous.)
Anyhow, we the rocks in the toaster oven, and none of the rocks were over 3 inches in size. 350 degrees is not really very hot. After a minute or two out of the oven they are not too dangerous should a kid bump or touch it. Important when planning a project for 5-6 year olds. With supervision it will be a good project for them.
Thanks again, Loraine