I screen printed a 3.5 x 3 piece meant to be a night light. It looks fine except the design isn't balanced. Because it's a roadrunner there's no way to cut it down to balance it without losing the tail. I have no idea why I didn't notice this before the last fuse. I just don't like it but imagine that I could use it as part of another, larger piece--e.g., a small plate. Originally, it was 3 mm clear fused ink side down over a 2 mm Bullseye base.
I would really appreciate to know if there's a way to salvage this? Many thanks,
Drewcilla
Help reusing fully fused piece
Moderators: Brad Walker, Tony Smith
-
lorimendenhall
- Posts: 91
- Joined: Wed Apr 10, 2013 8:54 pm
- Location: Orange County, CA
- Contact:
Re: Help reusing fully fused piece
I have not done this yet but I think it's fine to incorporate it into a new piece and full fuse again.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Help reusing fully fused piece
I throw things like that in a box until I am ready to do a pot melt or a pattern bar!
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Re: Help reusing fully fused piece
I'm with Laurie. That's what I do with my "Hall of Shame" items and it makes for some interesting results.Laurie Spray wrote:I throw things like that in a box until I am ready to do a pot melt or a pattern bar!