Drop Ring Vessel

Post by StaceyG »

After much trial and error, I have a presentable drop ring vessel. I used 4 layers of glass, and it dropped about 5". 3 layers was sometimes just a little too thin. I like the feel of the heavier vessel with 4 layers, so I think I will stick with that. The colors remind me of the beach, so I am really happy with how it all turned out.
Attachments
292989_4985746848518_1670455770_n.jpg
Eryc F.
Posts: 50
Joined: Sun Apr 28, 2013 8:29 am
Location: Canton, MA
Contact:

Re: Drop Ring Vessel

Post by Eryc F. »

That's really nice! And elegant!
Tracy Fries
Posts: 41
Joined: Thu Jun 14, 2012 7:14 pm

Re: Drop Ring Vessel

Post by Tracy Fries »

Lovely piece! Thank you for sharing.
la suisse
Posts: 26
Joined: Wed Jul 15, 2009 8:41 am

Re: Drop Ring Vessel

Post by la suisse »

This is beautiful and I really do love the colors!
Warren Weiss
Posts: 137
Joined: Thu Mar 13, 2003 8:06 pm
Location: Richmond, VA

Re: Drop Ring Vessel

Post by Warren Weiss »

Stacey,
Lovely work. What was the diameter of the hole in your drop ring? Thanks.
Warren
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: Drop Ring Vessel

Post by AndyT »

Way nice!
StaceyG
Posts: 40
Joined: Sun Feb 22, 2004 8:17 pm
Location: Baltimore, Maryland

Re: Drop Ring Vessel

Post by StaceyG »

The hole in the center is about 3".
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: Drop Ring Vessel

Post by Havi »

StaceyG wrote:The hole in the center is about 3".

And how tall is it.
A nice piece, I like it.
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
StaceyG
Posts: 40
Joined: Sun Feb 22, 2004 8:17 pm
Location: Baltimore, Maryland

Re: Drop Ring Vessel

Post by StaceyG »

Its about 5" high.
Drewcilla
Posts: 60
Joined: Fri Apr 11, 2008 9:10 am

Re: Drop Ring Vessel

Post by Drewcilla »

Lovely. Thanks for sharing.
Post Reply