"Unslump" a sushi dish?
Moderator: Tony Smith
-
susanmozingo
- Posts: 7
- Joined: Sun Jun 06, 2004 4:12 pm
"Unslump" a sushi dish?
I have a Bullseye COE90, eight inch, 6mm, fully fused and slumped sushi dish. I want to flatten the piece and fuse it again using a textured mold. Can I undo the slump easily and successfully? Thanks.
-
Barry Gitelson
- Posts: 31
- Joined: Sat Feb 07, 2009 8:28 pm
- Location: On the mountain side in Kona Hawaii
Re: "Unslump" a sushi dish?
I have unslumped a plate with a giant bubble before .... so my thought would be yes.
Barry Gitelson
Kona, HI
"Some dance to remember, some dance to forget" Hotel California - The Eagles
"Your talent is God's gift to you. What you do with it is your gift back to God." Author: Leo Buscaglia
Kona, HI
"Some dance to remember, some dance to forget" Hotel California - The Eagles
"Your talent is God's gift to you. What you do with it is your gift back to God." Author: Leo Buscaglia
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: "Unslump" a sushi dish?
Probably yes but it is often easier to make a new one. Why wreck a good dish?