Thanks
How many shelves can I use to fuse glass in my large skutt
Moderators: Brad Walker, Tony Smith
-
deborahbur
- Posts: 51
- Joined: Thu Apr 10, 2003 2:09 pm
- Location: Tiverton, Rhode Island
- Contact:
How many shelves can I use to fuse glass in my large skutt
I have a skutt ceramic kiln and am fusing and slumping glass. How many of my kiln shelves can I use to fuse glass and get an even fusing and slumping?
Thanks
Thanks
For larger pieces, like bowls at least 12", I can use three shelves and get away with good results. There is a noticeable difference between level of fusing although not quality of fuse. With small pieces like magnets, I use only two shelves to get consistency... with three, I can get spiking on the bottom shelf. I don't have zone control. In fact, I don't have a controller on the Skutt. I just fire my switches medium on all three levels and don't open the kiln until next morning. My idiot-proof firing program!
LOL,
Dani
LOL,
Dani
-
deborahbur
- Posts: 51
- Joined: Thu Apr 10, 2003 2:09 pm
- Location: Tiverton, Rhode Island
- Contact:
Are those 1/2 shelves staggered or full shelves
Are your shelves 1/2 shelves staggered or full shelves one on top of the other?
Thanks
Thanks
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
Lynne Chappell
- Posts: 186
- Joined: Fri Mar 14, 2003 2:05 am
- Location: Surrey B.C. Canada
- Contact:
In my ceramic kiln I use a full shelf (16") on the bottom, and a smaller shelf (13") on top. This gives me a consistent result on both shelves. If I use both full shelves, the lower shelf is cooler than the top shelf. OK if that is what you want, and I guess every kiln will have its own peculiarities.
Lynne
Lynne