Dichro frit?
Moderators: Brad Walker, Tony Smith
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Dichro frit?
Have some pieces of scrap Be Sizzle stix I'm wondering if I put these in the crusher what will be the result? Anyone done this? Will the dichroic coating stay intact in pieces?
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
Lynn Perry
- Posts: 129
- Joined: Sun Jun 08, 2003 5:27 pm
- Location: East Tennessee
Re: Dichro frit?
Jim, the coating remains mostly intact but some very fine coating will detach. I have never purchased the frit pre-coated from CBS which has more coating on the surface, but making my own frit worked fine for my project.
Lynn Perry
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Dichro frit?
well I'll give it a try and see thanks
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
David Jenkins
- Posts: 174
- Joined: Wed Apr 29, 2009 10:35 pm
- Location: Cypress, Texas
Re: Dichro frit?
I got some dichro frit (can't remember where, now) and was disappointed with results using it. It had been created by crushing/breaking dichro sheets, and hence each piece had a significant surface area that was not coated. When I fused it as a decoration, there was was very little of exposed coating, and it performed simply as coarse frit of the base glass would have done. I thought (briefly) of trying to align the pieces so that the coating was up, but quickly realized that the randomness of the frit creation made that impossible.
I'd be interested if others have techniques for creating/using dichro frit that will allow each piece to expose its coating to the fullest - is such a thing possible?
I'd be interested if others have techniques for creating/using dichro frit that will allow each piece to expose its coating to the fullest - is such a thing possible?
Dave Jenkins
Glass at Harbor Gates
Cypress, TX
Glass at Harbor Gates
Cypress, TX
-
lorimendenhall
- Posts: 91
- Joined: Wed Apr 10, 2013 8:54 pm
- Location: Orange County, CA
- Contact:
Re: Dichro frit?
well CBS is now selling dichro dust, but it's very pricey. otherwise there would be no way to actually make sure the dichro side of frit is facing up, I mean how would you do that??? this is why I don't use dichro frit, even though I am a huge dichro fan.
Last edited by lorimendenhall on Thu Jul 04, 2013 4:20 pm, edited 1 time in total.
Re: Dichro frit?
CBS dichroic has a film placed onto a copper substrate that slips right off the copper if you roll a hot bubble across it. Often sections of this come off and are lose inside the plastic bag. This thicker than usual film would make nice fairy dust.
Re: Dichro frit?
The disadvantage with making dichro frit, is that it is only coated on one side, so when you fuse you don't have control of where the dichro is (although it could be an interesting look) CBS coats the frit on all sides, so you always have dichro showing
-
carol carson
- Posts: 58
- Joined: Sat Jul 30, 2005 6:25 pm
- Location: Portland OR
- Contact:
Re: Dichro frit?
I've made my own and used it in a night sky piece. Even though it was only coated on the one side, I liked the dimension it gave with some of it reflecting brightly and some very subtly. So it may depend on what you are going to use it for. The ready made stuff is very expensive (and a bit garish for my own personal taste).