BE reactive ice irid

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

BE reactive ice irid

Post by Nina Falk »

How much does the irid coating diminish the reaction?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: BE reactive ice irid

Post by Brad Walker »

Depends on the temperature you fire to. High enough and it makes no difference. Lower and you can get some interesting effects, especially with irid down against a copper glass.

See magnets #6 and #12 from this year's magnet exchange: http://warmglass.com/magnet/2013%20Magn ... 040113.pdf
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: BE reactive ice irid

Post by Nina Falk »

thanks, Brad. I am curious to know what she used for #6.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: BE reactive ice irid

Post by Brad Walker »

Nina Falk wrote:thanks, Brad. I am curious to know what she used for #6.
Same as #12, just without the layer on the very bottom.
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: BE reactive ice irid

Post by Nina Falk »

sorry, I meant #12. that's turquoise opal, capped with reactive ice? or turquoise opal with reactive ice powder?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: BE reactive ice irid

Post by Brad Walker »

Nina Falk wrote:sorry, I meant #12. that's turquoise opal, capped with reactive ice? or turquoise opal with reactive ice powder?
The How-Tos discuss how #12 was made. Just check the details out in the pdf. It starts on page 16.
Nina Falk
Posts: 116
Joined: Sun Jan 16, 2005 1:57 pm
Location: Takoma Park, Maryland
Contact:

Re: BE reactive ice irid

Post by Nina Falk »

Thanks Brad.
Post Reply