Glue!
I've made a large panel and it's too big to fuse together in my kiln. It's 25" high and about 10 pieces that all fit together. It's some clear and some opal. I thought about use a piece of 1/4" float and gluing all pieces to it. Since there is opal, I can't use UV glue. I want something that will hold and not yellow. Any suggestions?????
Greg
-
Tyler Frisby
- Posts: 75
- Joined: Tue Dec 02, 2003 8:27 pm
- Location: Canada
-
Barbara Cashman
- Posts: 151
- Joined: Sun Mar 09, 2003 5:42 pm
- Location: Greensboro NC
- Contact:
-
RiverWoman
- Posts: 1
- Joined: Mon Mar 15, 2004 10:31 pm
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
I've never used it myself, but it came recommended to me, 2 part silicone. There is a long working time. You do need to put it in a vacuum chamber to get rid of bubbles.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions