I have been experimenting for a year now with inconsistent results fusing and melting plateglass in molds I am at a point of experimenting with using crucibles and doing a full melt. I have come across several references in this forum of using clay flower pots. My question Would this be an option and how well will it work? If this s a useable option then how large of a clay pot is useable in this manner?
Ron
Casting telescope mirrors
Moderator: Tony Smith
-
Wendell Brown
- Posts: 8
- Joined: Sun Jul 21, 2013 10:48 am
Re: Casting telescope mirrors
http://www.mdpub.com/scopeworks/blanks/index.html has been fusing glass for sometime. Check it out.
-
Ron Behrens
- Posts: 38
- Joined: Wed Jul 24, 2013 8:07 pm
Re: Casting telescope mirrors
That was one of the first sites I came across roughly a year ago. Lots of useful info that I have used. I however want to go further and cast from a full melt in a crucible---- to learn if nothing elss---- and hoping it gives me a cleaner glass result
Ron
Ron
-
Wendell Brown
- Posts: 8
- Joined: Sun Jul 21, 2013 10:48 am
Re: Casting telescope mirrors
Up to what diameter blank are you trying to get to? I will watch this thread to learn also. These members have lots of experience and ideas.
-
Ron Behrens
- Posts: 38
- Joined: Wed Jul 24, 2013 8:07 pm
Re: Casting telescope mirrors
I am currently working on 12 and 18 in diameter and up to 2.5 in thick. Once I get this down pat I will go up to 32 and 36
In diameter. I also plan to slump the blank over a prepared mold and create a meniscus blank
Ron
In diameter. I also plan to slump the blank over a prepared mold and create a meniscus blank
Ron