I have a question about a schedule for a soft fuse. It's a 12" square with a Santa Clause cut out on top; it's all 96 glass. I sprintkle coarse frit around the Santa. On the Santa hat I put on two holly leaves (cut in half) with three red berries - one on each of the leaf ends and one on top of the white part of the hat. I have a Skutt 14" Square with the elements in the top. I know that I must allow for extra time for the berries and holly as this makes it an uneven depth. I can't upload a picture as the file is too big. Can anyone suggest a schedule that will allow for the extra annealing time?.
Thanks so much for your help. I really appreciate this board. Also, thanks to whoever recommended using an air gun to get the bolt off my tile saw so I could use my glass blade. It was really stuck on there. It took longer to hook up the compressor and gun than it did to get if off.
Patty
Scheduling question
Moderators: Brad Walker, Tony Smith
Scheduling question
Patty
It often shows a command of language to say nothing - author unkown.
It often shows a command of language to say nothing - author unkown.
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Scheduling question
2 questions
Is the base 2 layers of glass? That will determine how hot you can take it for the look
you want.
Do you want the berries etc to fuse fully or remain raised?
Is the base 2 layers of glass? That will determine how hot you can take it for the look
you want.
Do you want the berries etc to fuse fully or remain raised?
Last edited by Laurie Spray on Sun Aug 04, 2013 11:46 am, edited 1 time in total.
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: Scheduling question
If you go into your photo program on your computer it is usually easy to downsize pics so they will post here.
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
Re: Scheduling question
Laurie,
No, the base is one layer with the coarse frit and Santa as the second. The holly on the hat is two leaves cut in half with the berries on it. So, that makes four, right, but just in that one spot which causes the unevenness. That's what I have to anneal for if I'm correct.
Thanks about the photo edit idea. I'll try it. There's so many things to learn
Patty
No, the base is one layer with the coarse frit and Santa as the second. The holly on the hat is two leaves cut in half with the berries on it. So, that makes four, right, but just in that one spot which causes the unevenness. That's what I have to anneal for if I'm correct.
Thanks about the photo edit idea. I'll try it. There's so many things to learn
Patty
Patty
It often shows a command of language to say nothing - author unkown.
It often shows a command of language to say nothing - author unkown.
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Scheduling question
A simple rule of thumb that does not always work Qom course, is to anneal for about wide the thickest part of the piece. You can look up th s heddles for thick pieces on the bullseye site (they apply to any glass)
http://www.bullseyeglass.com/methods-id ... slabs.html
http://www.bullseyeglass.com/methods-id ... slabs.html
Steve Richard
You can view my Blog at: http://verrier-glass.blogspot.com/
You can view my Blog at: http://verrier-glass.blogspot.com/
Re: Scheduling question
Thanks Steve,
I finally did that! Should have done it to begin with, but, of course, didn't. It's in the kiln now.
Patty
I finally did that! Should have done it to begin with, but, of course, didn't. It's in the kiln now.
Patty