CoreLite Kiln Shelves

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Nbolinger
Posts: 5
Joined: Wed Dec 06, 2006 2:43 pm

CoreLite Kiln Shelves

Post by Nbolinger »

Can CoreLite kiln shelves be used with glass? Are they easy to cut if the size needs to be trimmed down from a larger shelf?
Tracy Fries
Posts: 41
Joined: Thu Jun 14, 2012 7:14 pm

Re: CoreLite Kiln Shelves

Post by Tracy Fries »

I use them. I purchased from Seattle Pottery and they happily cut them to size before shipping.
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: CoreLite Kiln Shelves

Post by Brad Walker »

Nbolinger wrote:Can CoreLite kiln shelves be used with glass? Are they easy to cut if the size needs to be trimmed down from a larger shelf?
They work fine with glass and can be cut with a tile saw just like a regular mullite/cordierite shelf. It's better if you cut across the hollow pockets, rather than parallel to them.
pgegen
Posts: 1
Joined: Thu Sep 08, 2005 11:56 pm
Location: Wichita, KS

Re: CoreLite Kiln Shelves

Post by pgegen »

Corelite shelves work fine for glass. The lighter weight is a real plus.

Just a reminder, the recommended heating and/or cooling rate for corelite shelves is only 200 degrees per hour.
dee
Posts: 302
Joined: Tue Mar 11, 2003 5:20 pm
Location: Atlanta GA
Contact:

Re: CoreLite Kiln Shelves

Post by dee »

i have corelite kiln shelves for my "papa" kiln and love them! i do ramp up 366 dph on initial firings and 250 dph for slump firings w/o a problem.
D
Dee Janssen
Unicorn's Creations Studio
http://ucjewelry.com
dee@ucjewelry.com
Yardic Glassworks
Posts: 80
Joined: Sat Mar 06, 2010 9:29 am

Re: CoreLite Kiln Shelves

Post by Yardic Glassworks »

I have 3 that I use consistently. I have found that they do not like pot melts, but I love them for everything else.
Tim Yardic
Yardic Glassworks
Post Reply