halo lustre
Moderators: Brad Walker, Tony Smith
halo lustre
does anyone know if there is a current supplier? I love this stuff but have had no luck finding any in the past 2 years.
"Every artist was first an amateur."
--Ralph Waldo Emerson
--Ralph Waldo Emerson
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: halo lustre
As far as I know, it's no longer being made.
When Engelhard was purchased by BASF around half a dozen years ago, the Hanovia division of Engelhard (which made the Halo lusters) was shut down. I believe Duncan still makes some of the gold lusters, but no one that I'm aware of makes anything like the Halo.
A real shame, because it was a great product.
When Engelhard was purchased by BASF around half a dozen years ago, the Hanovia division of Engelhard (which made the Halo lusters) was shut down. I believe Duncan still makes some of the gold lusters, but no one that I'm aware of makes anything like the Halo.
A real shame, because it was a great product.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: halo lustre
I would ask if Hereaus is making it. They are currently in the Lustre business. They bought Engelhard from BASF in 2009. I see no mention of halo, but they do do marble.
http://heraeus-preciouscolours.de/media ... =125853006
http://heraeus-preciouscolours.de/media ... =125853006
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: halo lustre
I asked Heraeus a while back and they said they weren't making a Halo product. That may have changed, but I have my doubts.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: halo lustre
Do we have any chemists in the house who can figure out how to alter an available lustre to do the halo thing?Brad Walker wrote:I asked Heraeus a while back and they said they weren't making a Halo product. That may have changed, but I have my doubts.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Re: halo lustre
I just googled it - and am not sure if this is the same thing, but try:
http://www.seattlepotterysupply.com/Mer ... ode=HHLAHM
Barb
http://www.seattlepotterysupply.com/Mer ... ode=HHLAHM
Barb