Thanks to Lauri Levanto, we have a preliminary draft of an online dictionary of kiln-forming terms. Please check it out and let us know what you think.
This is a draft, not a final version, so comments are encouraged. If you have suggestions for improvement, terms to add, or corrections, please note them in this thread.
Here's the page: http://www.warmglass.com/Dictionary-11.html
This is a draft, not a final version, so comments are encouraged. If you have suggestions for improvement, terms to add, or corrections, please note them in this thread.
Here's the page: http://www.warmglass.com/Dictionary-11.html
Last edited by Brad Walker on Tue Apr 20, 2004 9:06 am, edited 1 time in total.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Warm Glass Dictionary
Nice job Lauri!Brad Walker wrote:Thanks to Lauri Levanto, we have a preliminary draft of an online dictionary of kiln-forming terms. Please check it out and let us know what you think.
This is a draft, not a final version, so comments are encouraged. If you have suggestions for improvement, terms to add, or corrections, please note them in this thread.
Here's the page: http://www.warmglass.com/Dictionary-11.html
I read through and one of these days, I'll edit my idea of the changes, there are a few.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Stuart Clayman
- Posts: 224
- Joined: Mon Mar 31, 2003 12:35 pm
- Location: Virginia
- Contact:
Re: Warm Glass Dictionary
Thank you Lauri.. I have reviewed A, B, and C.Brad Walker wrote:Thanks to Lauri Levanto, please note them in this thread.
Base... the top piece is not always a pattern. It can be another color like Cathedral Pink over a light purple.
Binder.. there are also binders in Refractories ie fiber boards, fiber papers, thin fire, Vermiculite board ect. Sometimes these should be burned off first before using.
Blank.... does not have to be a cast piece ... sometimes the base piece is called a blank.
Cathedral.. often is not fusable wiht other colors of the same brand... Ouch thank goodness that is not true in Fusing glass, ie Bullseye fusable, Spectrum's, Uro's ect.
Compatability test...... tet should be test.
When I spend time on the rest of them, and look to see if others should be added would you like them in the thread or would you like me to e-mail them to you?
Stuart
-
Bev Brandt
- Posts: 50
- Joined: Mon Mar 10, 2003 11:35 am
- Location: St. Louis, MO
- Contact:
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Warm Glass Dictionary
Put them in this thread. We know the version of the dictionary is rough, but thought it'd be good to get lots of public input before we clean it up.Stuart Clayman wrote:When I spend time on the rest of them, and look to see if others should be added would you like them in the thread or would you like me to e-mail them to you?
After a while, we'll do a second version that will be cleaner. But first just document comments here so others can see and comment if needed.
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
-
Geri Comstock
- Posts: 340
- Joined: Mon Mar 10, 2003 4:16 pm
- Location: Northern CA
- Contact:
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
Thanks for comments
But we need MORE.
I'll pick them here and insert the necessary changes.
It was really a fun job - even in a foreign language
I learned a lot.
-lauri
I'll pick them here and insert the necessary changes.
It was really a fun job - even in a foreign language
I learned a lot.
-lauri
alumina: can it really be used for blasting?
annealing range: stree should be stress
s/jevelry/jewelry/
crystal: add hyperlink to lead glass
devit: chrystals should be crystals
dvell: should be dwell
flashing color: should be flashed glass
flux: couls should be could
grog: hyperlink chamotte
handrolled: vawy should be wavy
the second sentence of your definition of heat is incorrect, or at least very incomplete.
lost vax should be lost wax, unless you're talking about old dec computers.
definition of pattern bar is incomplete. it's not just rods or stringers. you can make them out of frit, wide pieces of sheet glass, and lots of other shapes of glass.
raku clay: bisquit should be bisque
rod: could be any size. i've seen 10" rods. it isn't even a shape, i've seen oval and square rods.
shard: doesn't have to be thin glass. shards of a car window, for instance, is pretty thick.
silicosis: maks should be mask
slip: clay GOO? how about liquified clay?
tempered: indutrially should be industrially
Translucent: translucent glass doesn't have to have a surface pattern.
Vitrigraph: should be vitreograph i think
wbs: should be a hyperlink to wet belt sander
good work bringing all these into one place.
annealing range: stree should be stress
s/jevelry/jewelry/
crystal: add hyperlink to lead glass
devit: chrystals should be crystals
dvell: should be dwell
flashing color: should be flashed glass
flux: couls should be could
grog: hyperlink chamotte
handrolled: vawy should be wavy
the second sentence of your definition of heat is incorrect, or at least very incomplete.
lost vax should be lost wax, unless you're talking about old dec computers.
definition of pattern bar is incomplete. it's not just rods or stringers. you can make them out of frit, wide pieces of sheet glass, and lots of other shapes of glass.
raku clay: bisquit should be bisque
rod: could be any size. i've seen 10" rods. it isn't even a shape, i've seen oval and square rods.
shard: doesn't have to be thin glass. shards of a car window, for instance, is pretty thick.
silicosis: maks should be mask
slip: clay GOO? how about liquified clay?
tempered: indutrially should be industrially
Translucent: translucent glass doesn't have to have a surface pattern.
Vitrigraph: should be vitreograph i think
wbs: should be a hyperlink to wet belt sander
good work bringing all these into one place.
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Warm Glass Dictionary
Corrections on BOLDBrad Walker wrote:Thanks to Lauri Levanto, we have a preliminary draft of an online dictionary of kiln-forming terms. Please check it out and let us know what you think.
This is a draft, not a final version, so comments are encouraged. If you have suggestions for improvement, terms to add, or corrections, please note them in this thread.
Here's the page: http://www.warmglass.com/Dictionary-11.html
Bentonite can b used as suspension agent
Calcium Carbonate Ca CO3 whiting
Calcium Oxide Ca O Lime
plaster of paris Ca O4 . 1/2 H2 O
O is oxigen
Cerium Cerium oxide used for fine polishing. note if U can feel scratch with ur nail use pumace first, clean up then use cerium, keep wheel damp with cloth
Colloidal When a material is mixed with a liquid in so small particles that these do not settle to the bottom. Some colored glasses are made with colloidal metals that interfere with the light producing color. Two liquids can form a colloin COLLOID like in mayonnaise
Compatibility test To test compatibility pieces of different glass are full fused on a base glass. The tet TEST piece may show fractures - not compatible - or stress when viewed with a polariscope
Devitrification
Devit Result of devitrification. When glass is made the chrystalline ingredients are vitrified,melted to a liquid form. Devit is reverse of this process when chrystals form on OR WITHIN glass. Devit can be prevented or reduced by using oversprays.
Devit is glass molecules arranged in ordely fashion micro cristaline or larger cristals or both
In our normal glass the molecules R arranged in a random manner ( with some glasses this is not true )
Anti devit stuff works by making the glass 2 liquid so the cristals cant grow, also it will tend 2 disolve any neucleation points, so again it cant grow
Devit will only grow within a certain viscosity range, to stiff or 2 liquid n it cant grow
It also needs something 2 grow from like dirt or a scratch ( neucleation point )
It is this reason that devit usually only grows at an interface
Anty devit applied 2 light devit will mask it as it will B shiny n there may B a little disolving going on depending on temps
Devit usually incompatable but is OK up to a crertain size ( varies from glass 2 glass
Evenity EVENIVITY A WG term that refers to the uniformity of temperature in the kiln.
Flux use of can B used 2 stick glass together n assist in melting at a lower temp
Used 2 lower melt temp of colourants body stains on glaze
Body Stain
On Glaze
Glass enamel
Frit 1. Glass that has been crushed to small grains.
2. Ceramics: a composite powder used in glazing. Some toxic or otherwise difficult ingredients are enetered into the glaze mix as frit.
Frit is also a term used where a mixture of materials is heated whereby all the gassing n reactions r finished
This is then quenched n ground
Body stains, enamels, on glaze R made this way, it is usual 2 fire these much lower when manufactured
The advantage is that no or little gassing / reactions happen buring use
These can then B further softened with flux
Lapwheel UK - flat bed grinder
Opal Glass that is opaque or milky. See transparent and translucent can have cryistals with in it so can change on reheat ( devit troughout )
Peeking Visually monitoring the process in the kiln, with out opening the door so kiln not cool
Rigidizer Used to harden or rigidize forms made of soft ceramic fiber material colloidal alumina or colloidal silica SiO2
Neucleation point Something that devit grows from this can B dirt , scratch, or something cristaline see also devit
Striking A glass that is made like this can discolour on refiring
Bullseye uses this term to describe class that obteins the final color only after a second firing ,

definition
the dictionary is great,,,wonderful idea,,,there is nothing under letter Y,,,here is suggestion
yee ha..... the tern used when at last the problem is solved, quickly followed by "its about time" or "now what"
yee ha..... the tern used when at last the problem is solved, quickly followed by "its about time" or "now what"
-
Brian and Jenny Blanthorn
- Posts: 353
- Joined: Mon Mar 10, 2003 5:25 pm
- Location: UK
- Contact:
Re: Warm Glass Dictionary
Aussie Roll-Up Developed by Australians Schott Chaseling /and Kirstie Rea.Brad Walker wrote:Thanks to Lauri Levanto, we have a preliminary draft of an online dictionary of kiln-forming terms. Please check it out and let us know what you think.
This is a draft, not a final version, so comments are encouraged. If you have suggestions for improvement, terms to add, or corrections, please note them in this thread.
Here's the page: http://www.warmglass.com/Dictionary-11.html
A combination of kiln working and hot glass where glass is first made in the kiln then picked up / rolled up, then worked using hot glass techniques
Roll-Up See Aussie Roll-Up
Brian

-
charlie holden
- Posts: 260
- Joined: Thu Mar 13, 2003 8:26 pm
- Location: Atlanta
I know everybody else thinks it's a crazy idea but I'll try anyway.
If you put the dictionary on Wiki software everybody could edit it directly. It is up to the community to police the posts.
wiki.org/wiki.cgi?WhatIsWiki
Look at the wikipedia for an example of wiki on a large scale.
wikipedia.org
ch
If you put the dictionary on Wiki software everybody could edit it directly. It is up to the community to police the posts.
wiki.org/wiki.cgi?WhatIsWiki
Look at the wikipedia for an example of wiki on a large scale.
wikipedia.org
ch
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Maybe I'm old-fashioned, but the thought of over a hundred people editing the same document is enough to make me shudder. Have you participated in this wiki thing before?charlie holden wrote:If you put the dictionary on Wiki software everybody could edit it directly. It is up to the community to police the posts.
-
Lani McGregor
- Posts: 121
- Joined: Mon Mar 10, 2003 2:12 pm
- Location: Portland, OR
- Contact:
I think this is a fantastic opportunity for a lot of much-needed discussion/debate on terminology.
Thanks, Lauri!
PS. Charlie, it's "vitrigraph". I can be inflexible on this point, since I coined the term and wrote the first print material detailing the process (Bullseye's TechNotes #2, Copyright 1995)
I specifically chose the "i" so as not to confuse it with..
Vitrograph or vitreography, which is printing with glass plates, see Littleton among others.
On this note, I think it would be helpful along with the definitions to provide some historical attribution as to where processes etc. developed (not to overlook the Egyptians et al as innovators of combing. And Aussies for the roll-up etc.)... OK, this one's got me energized!
Thanks, Lauri!
PS. Charlie, it's "vitrigraph". I can be inflexible on this point, since I coined the term and wrote the first print material detailing the process (Bullseye's TechNotes #2, Copyright 1995)
I specifically chose the "i" so as not to confuse it with..
Vitrograph or vitreography, which is printing with glass plates, see Littleton among others.
On this note, I think it would be helpful along with the definitions to provide some historical attribution as to where processes etc. developed (not to overlook the Egyptians et al as innovators of combing. And Aussies for the roll-up etc.)... OK, this one's got me energized!
In a Wiki, when a user clicks on the "Edit" link on a page the page is locked so no one else can edit it. Of course you have to think about someone 'leaving' the edit page (say, exiting their browser) without releasing the lock (or leaving the page in edit mode and walking away). In that case you'd have to wait for the lock time period to expire. I believe the default is one hour and I don't know if you can change it. Seems like you'd also want to limit editing to registered board users. We use Twiki (http://www.twiki.org) on our project - it's a fairly mature Wiki implementation.Brad Walker wrote:Maybe I'm old-fashioned, but the thought of over a hundred people editing the same document is enough to make me shudder. Have you participated in this wiki thing before?charlie holden wrote:If you put the dictionary on Wiki software everybody could edit it directly. It is up to the community to police the posts.
Ed
------------------------------------
Gratitude.Respect.Responsibility.
Gratitude.Respect.Responsibility.
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
To Lani
Great you joined in.
1. I have discussed with Brad that it is possible to link further into archives. F.ex:
Powder wafer - (definition) Read further (link to Bob leatherbarrow*s posting.
This will take time to find out proper postings.
2. As I have a limited access to original sources
. living in countruside, Finland - I'll not
infringe copyrights. The reader has better to directly consultate
Charles Bray: Dictionary of glass.
-lauri
1. I have discussed with Brad that it is possible to link further into archives. F.ex:
Powder wafer - (definition) Read further (link to Bob leatherbarrow*s posting.
This will take time to find out proper postings.
2. As I have a limited access to original sources
. living in countruside, Finland - I'll not
infringe copyrights. The reader has better to directly consultate
Charles Bray: Dictionary of glass.
-lauri
-
Lauri Levanto
- Posts: 270
- Joined: Tue Mar 11, 2003 7:33 am
- Location: Halikko, Finland
Wikipedia
I know the wikipedia, though I have no hands on experience on it. It was in my mind to put the dictionary in it.
As Brad mentioned, 100 persons editing the draft
may cause more confusion. maybe when we have something
stabilized...
The greatest worry is forth and back editing. We have already arguments about the term frit.
One more point is language. Now I have used three languages; English, UK English and Brianese which
may be unitelligle to people putside WG boad.
Including Aussie, Pidgin English etc may run to a chaos.
As there already exists the Bray: Dictionary of glaa
my purpose was to help with the colloqial forms of WG board.
-lauri
-lauri
As Brad mentioned, 100 persons editing the draft
may cause more confusion. maybe when we have something
stabilized...
The greatest worry is forth and back editing. We have already arguments about the term frit.
One more point is language. Now I have used three languages; English, UK English and Brianese which
may be unitelligle to people putside WG boad.
Including Aussie, Pidgin English etc may run to a chaos.
As there already exists the Bray: Dictionary of glaa
my purpose was to help with the colloqial forms of WG board.
-lauri
-lauri