A new tool for drawing with powder or fine Frit

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Sandpen
Posts: 6
Joined: Fri Sep 27, 2013 2:00 pm

Re: A new tool for drawing with powder or fine Frit

Post by Sandpen »

Hello Vicki!

Thanks for backing, we made a video with the glass powder and grain today: http://www.youtube.com/watch?v=Bnya0JWZoKI
Vicki M
Posts: 38
Joined: Sat Aug 30, 2003 10:56 am
Location: Canada

Re: A new tool for drawing with powder or fine Frit

Post by Vicki M »

Just watched the video, it looks so smooth to use. I have shared on my facebook too! Can't wait to get one. :D
AndyT
Posts: 171
Joined: Mon Apr 30, 2007 9:34 am
Location: Medford, Orygun
Contact:

Re: A new tool for drawing with powder or fine Frit

Post by AndyT »

JestersBaubles wrote:
Terry Ow-Wing wrote:Can you post a revies of the powder vibe? Do you have the original one or the 2nd version? Or you can pm me with your review if you feel more comfortable with that. I would appreciate the info. :)


Thanks - Terry
I ordered a powder vibe recently, and I'm just not feeling the love. I guess I need to give it another try ;).

Dana
I bought the Powder Vibe from D&L. Tried it several times and it's been in the box ever since.
Terry Ow-Wing
Posts: 124
Joined: Sun Mar 09, 2003 3:21 pm
Location: San Francisco, Ca.
Contact:

Re: A new tool for drawing with powder or fine Frit

Post by Terry Ow-Wing »

AndyT wrote:
JestersBaubles wrote:
Terry Ow-Wing wrote:Can you post a revies of the powder vibe? Do you have the original one or the 2nd version? Or you can pm me with your review if you feel more comfortable with that. I would appreciate the info. :)


Thanks - Terry
I ordered a powder vibe recently, and I'm just not feeling the love. I guess I need to give it another try ;).

Dana
I bought the Powder Vibe from D&L. Tried it several times and it's been in the box ever since.


Can you post what you did not like about it? Is it the 1st model with the plastic handle addition or the 2nd model with the slim pen like motor? thanks
Terry Ow-Wing Designs
Kilnformed and Lampworked Glass Art
http://GlassArt.weebly.com
Image
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: A new tool for drawing with powder or fine Frit

Post by Peter Angel »

With the powder vibe, the frit would stop flowing.

It would clog up at the outlet.

The solution was to unblock the clog by pushing a toothpick into the outlet, tapping it a few times, and then you would continue....until it blocked up again.
Peter Angel
http://peterangelart.blogspot.com/

A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
Post Reply