sink mold used for hanging light?
I am planning on making a dining room hanging light (this shape: http://www.artfulhome.com/product/Art-G ... Bowl/63171 or like this http://www.artfulhome.com/product/Glass ... Lamp/30427 ). Is a sink mold used to make these large lamps? (sink mold like this: http://www.fusionheadquarters.com/product_p/sinkmol.htm ). Unfortunately, I live in a rural area and have to order molds so I can't go and see them before I buy - any advice is appreciated!
thanks very much!
Jane
thanks very much!
Jane
Jane Morgan
Re: sink mold used for hanging light?
Instead of buying an expensive "sink mold" just look for a big wok. Or go to a metal spinner and see what they have to offer in stock. Much cheaper, just as good . . .
-
Jane Morgan
- Posts: 28
- Joined: Sat Sep 01, 2007 11:49 pm
- Location: Central Coast of California
Re: sink mold used for hanging light?
Brock: does the wok need to be stainless steel?Brock wrote:Instead of buying an expensive "sink mold" just look for a big wok. Or go to a metal spinner and see what they have to offer in stock. Much cheaper, just as good . . .
Jerry
Re: sink mold used for hanging light?
No, but SS is probably better. We used to travel with a dozen metal woks for teaching. I can't remember what they were but not SS. Basically, if it can take the heat it'll work. I slump at 1150.
Re: sink mold used for hanging light?
your first link reminds me of BE ball mold 008737. it has that nice rounded shape. it is only 20" though, so the final bowl will be a bit smaller. Still a very useful size for a lamp...mold is expensive, as Brock said.
cheers, seachange
cheers, seachange
-
Tom Fuhrman
- Posts: 187
- Joined: Mon Mar 10, 2003 11:44 am
- Location: eastern Tennessee
- Contact:
Re: sink mold used for hanging light?
I've been using a standard steel wok for over 10 years and who knows how many items I've slumped in it and still going strong. Think I paid about $30 for a 24" one when I got it many years ago. just put plenty of kiln wash on it and don't go too hot.Brock wrote:No, but SS is probably better. We used to travel with a dozen metal woks for teaching. I can't remember what they were but not SS. Basically, if it can take the heat it'll work. I slump at 1150.
Re: sink mold used for hanging light?
I also bought a wok about 8 or 9 years ago. I don't do sinks, but I use it for platters and trays. To slump, I fire 1350 for float and 1265 or so for 90 or 96.
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: sink mold used for hanging light?
304 stainless steel molds will last for your lifetime. I have reasons to fire as hot as 1420ºF, in mine, and they hold up just fine.
Eastman ss Woks are available in 2 sizes on Amazon. They have handles and a straight edge. You can remove or leave the handles in place. I would only remove them if space is an issue. These have a flat spot on the bottom which gives them a stability factor. I have a sink in my home, made this way, and it drains well enough. For a light fixture, you would have to stop the slump before it flattened out.
The advantage to the Fusion HQ molds is that they have a rolled top edge which makes the mold more stable. They also have good shapes.
Eastman ss Woks are available in 2 sizes on Amazon. They have handles and a straight edge. You can remove or leave the handles in place. I would only remove them if space is an issue. These have a flat spot on the bottom which gives them a stability factor. I have a sink in my home, made this way, and it drains well enough. For a light fixture, you would have to stop the slump before it flattened out.
The advantage to the Fusion HQ molds is that they have a rolled top edge which makes the mold more stable. They also have good shapes.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Jane Morgan
- Posts: 28
- Joined: Sat Sep 01, 2007 11:49 pm
- Location: Central Coast of California
Re: sink mold used for hanging light?
Thanks everyone - this is very helpful information.
Jane
Jane
Jane Morgan
Re: sink mold used for hanging light?
Woks work. Also check restaurant supply stores. They usually sell a huge range of stainless bowls and I've gotten some pretty big ones there. Heaven knows what they mix in them--maybe huge amounts of salad? Looking at woks and bowls gives you many more options for shape/depth.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
-
Laurie Spray
- Posts: 321
- Joined: Sat Dec 17, 2005 10:32 pm
- Location: SANTA CRUZ, CALIFORNIA
- Contact:
Re: sink mold used for hanging light?
I have a wok listed on our site under odds and ends....we have been doing a reorg and major studio clean out and have goodies from it for sale. I used to make sinks but not these days.
Just one large one listed.
Just one large one listed.
Laurie Spray
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
New website!! Http://bonnydoonfusedglasstools.com
Maker of stainless steel rings,pattern bar formers, pot melt pots, and Bottomless Molds
glass: http://lauriespray.blogspot.com
-
Jane Morgan
- Posts: 28
- Joined: Sat Sep 01, 2007 11:49 pm
- Location: Central Coast of California
Re: sink mold used for hanging light?
Thanks all!
Laurie - I sent you an email.
best,
Jane
Laurie - I sent you an email.
best,
Jane
Jane Morgan
Re: sink mold used for hanging light?
Curious if you have made this, would love to see a photo. How did you support it when drilling the holes and what type of hardware did you use?
-
Tom Fuhrman
- Posts: 187
- Joined: Mon Mar 10, 2003 11:44 am
- Location: eastern Tennessee
- Contact:
Re: sink mold used for hanging light?
I've had local potters make many large molds for me from either a porcelain body or stoneware and just have them bisque fire it. We had several style of sinks molds made this way and many times they are open to bartering for their clay pieces. Be sure and kiln wash the surface well.
-
Jane Morgan
- Posts: 28
- Joined: Sat Sep 01, 2007 11:49 pm
- Location: Central Coast of California
Re: sink mold used for hanging light?
Hi Stacy,
Unfortunately I've had a few unexpected things happen and I haven't yet had a chance to make it. I'll post pictures when I do, but you can see hardware examples at artfulhome.com
Jane
Unfortunately I've had a few unexpected things happen and I haven't yet had a chance to make it. I'll post pictures when I do, but you can see hardware examples at artfulhome.com
Jane
Jane Morgan
Re: sink mold used for hanging light?
Both great questions which I echo.StaceyG wrote:Curious if you have made this, would love to see a photo. How did you support it when drilling the holes and what type of hardware did you use?
I have been to numerous lamp supply stores looking for supply houses for lighting hardware with little success. Slumpys (board sponsor) has a limited number. Any suggestions out there?
Jerry
Re: sink mold used for hanging light?
You missed an opportunity, Brock: "If it'll take the heat, it'll wok."Brock wrote:No, but SS is probably better. We used to travel with a dozen metal woks for teaching. I can't remember what they were but not SS. Basically, if it can take the heat it'll work. I slump at 1150.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)