I have been testing Primo Primer, and like the results.  One thing I have noticed though, is the primer tends to "muck" up in my storage container.  I mix it in an old Gatorade bottle, put the marbles in it, and shake it up well.  If it sits for longer than a day, the primer separates from the water a bit, and mucks up in the bottom.
Any way to avoid this?
			
			
									
						
							Primo Primer Muck
Moderator: Tony Smith
- 
				Valerie Adams
 - Posts: 587
 - Joined: Mon Apr 19, 2004 2:49 pm
 - Location: Santa Rosa, California
 - Contact:
 
Re: Primo Primer Muck
I keep Bullseye's primer pre-mixed in a bottle too and it also separates. I just shake well before using. The ingredients are too heavy to stay suspended in water.
			
			
									
						
										
						- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: Primo Primer Muck
There is a primary difference between Bullseye primer and Primo primer.  In Bullseye the binder is kaolin EPK clay.  In Primo the binder is an organic gum.  These materials behave differently in the way they mix and disperse.
			
			
									
						
							Bert 
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
			
						Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
- 
				jim simmons
 - Posts: 478
 - Joined: Sun Mar 09, 2003 10:37 pm
 - Location: Hillsboro Oregon
 - Contact:
 
Re: Primo Primer Muck
Yea, but you can't avoid the separation
Jim
			
			
									
						
										
						Jim
Bert Weiss wrote:There is a primary difference between Bullseye primer and Primo primer. In Bullseye the binder is kaolin EPK clay. In Primo the binder is an organic gum. These materials behave differently in the way they mix and disperse.
Re: Primo Primer Muck
Bullseye primer separates just as nicely. I have both, side by side on a shelf, not much difference in appearance except for color.
			
			
									
						
							Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
			
						Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
- 
				Bert Weiss
 - Posts: 2339
 - Joined: Tue Mar 11, 2003 12:06 am
 - Location: Chatham NH
 - Contact:
 
Re: Primo Primer Muck
Kaoilin based primers are easier to remix than gum based.
			
			
									
						
							Bert 
Bert Weiss Art Glass*
http://www.customartglass.com