Fusing 19" dia. dichroic sheet to clear SPE 96

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
BobAde
Posts: 1
Joined: Tue Nov 05, 2013 3:58 pm

Fusing 19" dia. dichroic sheet to clear SPE 96

Post by BobAde »

How do I avoid trapping air bubbles when fusing this size material?
Brad Walker
Site Admin
Posts: 1542
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Fusing 19" dia. dichroic sheet to clear SPE 96

Post by Brad Walker »

BobAde wrote:How do I avoid trapping air bubbles when fusing this size material?
See this thread: http://www.warmglass.com/phpBB/viewtopi ... =2&t=40939

One additional comment -- if you fuse with the dichroic on top, you will have more trapped air bubbles than if you fuse with a thicker glass on top. That's because the thicker glass will help to push bubbles out.
Post Reply