Hello,
I am new to glasswork, but have access to the appropriate kilns and other resources to get started (I think). My first project sounded easy at first, but as I began to think through how to execute, I began to realize I need some help. Essentially, I would like to re-use beer bottle glass and slump it into a ~3/4" thick cylinder. It seems like HydroCal or HydroPerm might be the best materials to cast the mold with. Any other better materials? Assuming I can cast the mold the way I would like, my problem (likely among many I haven't thought of) is proper kiln settings and releasing the cylinder afterwards. I'm assuming I won't be able to reuse the mold and would have to break the mold. But how do I do that without breaking the glass? 
Any help or direction would be much appreciated. 
Thanks!
			
			
									
						
										
						New to glasswork, need help on a project
Moderator: Tony Smith
- 
				Graham Taylor
- Posts: 1
- Joined: Tue Nov 19, 2013 12:27 pm
- 
				Tom Fuhrman
- Posts: 187
- Joined: Mon Mar 10, 2003 11:44 am
- Location: eastern Tennessee
- Contact:
Re: New to glasswork, need help on a project
Get Henry Halem's Glass Notes book. he has a large section on casting and making molds. google Glass Notes ,Henry Halem and you can buy direct from him. lots of good info.
			
			
									
						
										
						Re: New to glasswork, need help on a project
Bottle glass is really hard to  melt into anything, you  picked a first project loaded with  pitfalls for a beginner. You  might want to visit a supplier of fusible glass or someone to help you through a casting. At least read lots more on this forum on casting projects. The  cost of the glass is tiny compared to the amount of work you are planning.
			
			
									
						
										
						Re: New to glasswork, need help on a project
I foresee a long journey ahead. 
Halem's book is a good start. I'd also suggest Kervin/Fenton's Pate de verre and kiln casting of glass. Excellent book on casting and it'll give you a bit of help with schedules as well.
			
			
									
						
							
Halem's book is a good start. I'd also suggest Kervin/Fenton's Pate de verre and kiln casting of glass. Excellent book on casting and it'll give you a bit of help with schedules as well.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
			
						Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
- 
				Peter Angel
- Posts: 186
- Joined: Fri Oct 31, 2008 9:26 am
- Location: Newtown, Sydney, Australia.
Re: New to glasswork, need help on a project
Peter Angel
http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.
			
						http://peterangelart.blogspot.com/
A bigger kiln, A bigger kiln, my kingdom for a bigger kiln.