Safety relating to thin fire kiln shelf paper
Moderators: Brad Walker, Tony Smith
Safety relating to thin fire kiln shelf paper
I Have acute contact dermatitis.  I work with glass and the kiln at least 5 days a week.  I have the dermatitis on my hands and wrists.  I do use rubber gloves when removing the kiln shelf paper which is very dusty, also a mask.  Has anyone come across this before?  Any suggestions on other forms of protection.  Thanks for any help.  Carol Ann
			
			
									
						
							Carol Ann
			
						Re: Safety relating to thin fire kiln shelf paper
Could be. Could also be a sensitivity to the gloves, particularly if they're latex and/or you're wearing them so long they're getting sweaty inside. I have a friend who discovered her latex sensitivity by wearing rubber-coated gloves when scraping kilnshelves and such. She developed welts all along the areas that exposed latex and once the reaction started, just about anything would make it worse. So first off, I'd see an allergist and make sure that there's not something else going on. You'll want to log everything that the affected areas come in contact with--change of soap or lotion (and, BTW, if you're in a flare-up, be really careful of which hand creams and such that you use--they can make it worse).
Then try taking a week off and staying away from the studio to see if the dermatitis goes away. Once your skin settles down, try not using shelf paper and see if the problems return. Kilnwash is cheaper and works just as well tho it's a bit more work. You'll want to vacuum out the kiln to remove any shelf paper residue, at least a couple of times over the course of a couple of days, because the dust drifts and resettles. Try that for at least a week, or as long as it takes for the allergic response to return.
If you discover you really are reacting to shelf paper and for some reason must use it anyway, swap gloves--look for surgical gloves for people with sensitive skin. Wear long-sleeved, high-necked shirts and pull the gloves OVER the sleeves to prevent dust getting to your skin.
If your studio is adjacent to your living spaces, keep the door to your studio closed when you're working, and put a change of clothes or a bathrobe and slippers right outside the studio. When you've finished for the day, take your outer clothes and shoes off IN the studio, stick 'em in a plastic bag or whatever and change into the robe and slippers (or whatever). This helps to keep the dust from tracking into the rest of the house, so that you have a respite from it.
			
			
									
						
							Then try taking a week off and staying away from the studio to see if the dermatitis goes away. Once your skin settles down, try not using shelf paper and see if the problems return. Kilnwash is cheaper and works just as well tho it's a bit more work. You'll want to vacuum out the kiln to remove any shelf paper residue, at least a couple of times over the course of a couple of days, because the dust drifts and resettles. Try that for at least a week, or as long as it takes for the allergic response to return.
If you discover you really are reacting to shelf paper and for some reason must use it anyway, swap gloves--look for surgical gloves for people with sensitive skin. Wear long-sleeved, high-necked shirts and pull the gloves OVER the sleeves to prevent dust getting to your skin.
If your studio is adjacent to your living spaces, keep the door to your studio closed when you're working, and put a change of clothes or a bathrobe and slippers right outside the studio. When you've finished for the day, take your outer clothes and shoes off IN the studio, stick 'em in a plastic bag or whatever and change into the robe and slippers (or whatever). This helps to keep the dust from tracking into the rest of the house, so that you have a respite from it.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
			
						Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
- 
				Kevin Midgley
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Safety relating to thin fire kiln shelf paper
Candida fungus loves to live inside damp rubber gloves.  
 
Hands must be kept absolutely dry.
Don't ever put damp hands inside a glove.
If you have no nail cuticles and that isn't from manicure treatments, and often get hangnails, it could be another source of the problem. 
   
 
over the counter fungicidal cremes can work.
My guess is it is problem you have since you live in your gloves.
After all that, ditch the paper. I've never used it.
			
			
									
						
										
						 
 Hands must be kept absolutely dry.
Don't ever put damp hands inside a glove.
If you have no nail cuticles and that isn't from manicure treatments, and often get hangnails, it could be another source of the problem.
 
   
 over the counter fungicidal cremes can work.
My guess is it is problem you have since you live in your gloves.
After all that, ditch the paper. I've never used it.
Re: Safety relating to thin fire kiln shelf paper
Kevin makes a really good point. I must wear gloves throughout the casting process (my hands become really irritated by the plasters), and if I wore the same pair of gloves for the whole day my hands would be a mess. I make a point of stripping off my gloves every half hour or so, letting my hands dry a bit (with or without washing them), and then putting on fresh. It makes a difference.
I'm not sure that's the problem here since your wrists are involved and I would think they'd be more likely to have air circulation, but that certainly could be a factor.
			
			
									
						
							I'm not sure that's the problem here since your wrists are involved and I would think they'd be more likely to have air circulation, but that certainly could be a factor.
Cynthia Morgan
Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
			
						Marketeer, Webbist, Glassist
http://www.morganica.com/bloggery
http://www.cynthiamorgan.com
"I wrote, therefore I was." (me)
Re: Safety relating to thin fire kiln shelf paper
So changing gloves and removing them periodically will be helpful.  I think more of the problem is the kiln shelf paper.
If you use kiln shelf paper, when you remove it, what is your process? I have a large kiln 56"x30", so after the firing when I remove the thin fire paper, the dust particles are hard to contain. The mask is essential, but how do you control the dust?
Do you vacuum the whole thing up. my usual process is to use wet paper towels to remove the paper. Is there a more efficient way to accomplish this? thanks for any recommendations.
			
			
									
						
							If you use kiln shelf paper, when you remove it, what is your process? I have a large kiln 56"x30", so after the firing when I remove the thin fire paper, the dust particles are hard to contain. The mask is essential, but how do you control the dust?
Do you vacuum the whole thing up. my usual process is to use wet paper towels to remove the paper. Is there a more efficient way to accomplish this? thanks for any recommendations.
Carol Ann
			
						- 
				Kevin Midgley
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Safety relating to thin fire kiln shelf paper
rainbow vacuum cleaners are low rated by consumer tests but they really do work to collect the dust in their water bowl.  As previously noted I don't use the shelf paper in my kilns however the regular fine studio dusts will turn into a thickened sludge when I do a heavy cleaning.   If you could pick one up used for $50 or $100 it could be a better paper picker upper. New, they go for a ridiculous $2000.   The rainbows are messier than a dry bag less vacuum but they work.  For sure, don't expect a septic system to like the contents and I dump mine in a composting area outside.
As far as drying off hands, I've ensured mine are completely cuticle dry by using a hair dryer on them.
			
			
									
						
										
						As far as drying off hands, I've ensured mine are completely cuticle dry by using a hair dryer on them.
- 
				Brad Walker
- Site Admin
- Posts: 1537
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Safety relating to thin fire kiln shelf paper
The main thing is a vacuum with a HEPA filter. They are available for many different shop vacs, as well as some home vacuums. A HEPA (High Efficient Particulate Air) filter will remove 99.7% of the particulates under 0.3 microns. These are the very small particles that can cause trouble when breathed.Carol Ann wrote:Do you vacuum the whole thing up. my usual process is to use wet paper towels to remove the paper. Is there a more efficient way to accomplish this? thanks for any recommendations.
To be extra safe, you could also wear a P100 respirator when cleaning up. The P100 is also a HEPA filter.
Re: Safety relating to thin fire kiln shelf paper
thanks.  I do have a HEPA filter on my vacuum cleaner.  I will use that to vacuum up the kiln paper.  
Also I will get your recommended respirator. thanks for your recommendations.
			
			
									
						
							Also I will get your recommended respirator. thanks for your recommendations.
Carol Ann
			
						Re: Safety relating to thin fire kiln shelf paper
Or you could use kiln wash and not worry about all this stuff.
			
			
									
						
										
						- 
				Kevin Midgley
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Safety relating to thin fire kiln shelf paper
I'm with you Brock, I cannot understand why someone would want to burn stuff in their kilns.  
For one it is expensive and if you take into account all the cleanup issues and time involved, applying kiln wash is simpler and quicker.
For two, if you are burning stuff in your kiln, it has to have an impact on the life of kiln elements. Add that into the cost and using the paper is insane.
For Three, burning thin fire paper necessitates venting of the kiln or gives you dirty fired glass which means you waste energy and have to attend the kiln to close it after burning has finished. Plus you have to deal with the stinky fumes.
For Four, what impact is there in the kiln and glass of having cold external air entering the kiln during the venting process? How many marginally annealed
pieces have been broken reaching 1000f as a result?
			
			
									
						
										
						For one it is expensive and if you take into account all the cleanup issues and time involved, applying kiln wash is simpler and quicker.
For two, if you are burning stuff in your kiln, it has to have an impact on the life of kiln elements. Add that into the cost and using the paper is insane.
For Three, burning thin fire paper necessitates venting of the kiln or gives you dirty fired glass which means you waste energy and have to attend the kiln to close it after burning has finished. Plus you have to deal with the stinky fumes.
For Four, what impact is there in the kiln and glass of having cold external air entering the kiln during the venting process? How many marginally annealed
pieces have been broken reaching 1000f as a result?
- 
				bob proulx
- Posts: 186
- Joined: Tue Dec 29, 2009 7:13 pm
- Location: Nahant Massachusetts
- Contact:
Re: Safety relating to thin fire kiln shelf paper
I agree with Brock, I find no reason to use the stuff.
Bob
			
			
									
						
										
						Bob
- 
				Greg Rawls
- Posts: 147
- Joined: Sun Mar 09, 2003 8:11 pm
- Location: Charleston, SC
- Contact:
Re: Safety relating to thin fire kiln shelf paper
Main ingredients in Thin Fire Paper are Cellulose, Aluminum Hydroxide, fiber glass, organic binders. It is predominately a nuisance dust and an irritant. Regarding the Fiber glass – the jury is out on toxicology but would be a good idea to wear a P95 respirators (cheaper than P100, less breathing resistance - the difference in efficiency vs. P100 is almost negligible). Some kiln lining paper does contain RCF so read the MSDS (BE does not). Keep kiln closed when binders are burning off.
			
			
									
						
							Greg
			
						Re: Safety relating to thin fire kiln shelf paper
Greg,Greg Rawls wrote:Keep kiln closed when binders are burning off.
Kevin had just mentioned in his post to vent the kiln when the Thin Fire is burning. His reasons made sense (for a newbie) as much as yours. I guess the jury is still out on that one too?
Lucie
- 
				Greg Rawls
- Posts: 147
- Joined: Sun Mar 09, 2003 8:11 pm
- Location: Charleston, SC
- Contact:
Re: Safety relating to thin fire kiln shelf paper
Your choice. I like to keep the smell contained.lmartine wrote:Greg,Greg Rawls wrote:Keep kiln closed when binders are burning off.
Kevin had just mentioned in his post to vent the kiln when the Thin Fire is burning. His reasons made sense (for a newbie) as much as yours. I guess the jury is still out on that one too?
Lucie
Greg
			
						- 
				Lynn Perry
- Posts: 129
- Joined: Sun Jun 08, 2003 5:27 pm
- Location: East Tennessee
Re: Safety relating to thin fire kiln shelf paper
Thanks, Greg, for the clarification about P100 versus P95. I have a refillable P100 but don't use it that often (kind of defeats the purpose of even having it), because it has too much breathing resistance for me. I bought a ten-pack of 3M P95 dust masks at Lowe's yesterday based on your information in hopes they will be more comfortable plus I can discard the used ones for better hygiene.Greg Rawls wrote:Main ingredients in Thin Fire Paper are Cellulose, Aluminum Hydroxide, fiber glass, organic binders. It is predominately a nuisance dust and an irritant. Regarding the Fiber glass – the jury is out on toxicology but would be a good idea to wear a P95 respirators (cheaper than P100, less breathing resistance - the difference in efficiency vs. P100 is almost negligible). Some kiln lining paper does contain RCF so read the MSDS (BE does not). Keep kiln closed when binders are burning off.
Lynn Perry
			
						- 
				Glass Fever
- Posts: 29
- Joined: Sat Aug 04, 2007 11:08 pm
- Location: Chicago Suburbs
- Contact:
Re: Safety relating to thin fire kiln shelf paper
If you are wearing gloves when removing the used Thinfire, I wouldn't think your contact dermatitis would be from the dust. It may actually be from the gloves as mentioned previously. I am an RN, and I used to get a similar thing on the backs of my hands. I thought I was developing a latex sensitivity. Turns out it was just the powder in the gloves. When I switched to powder free gloves the problem went away.
			
			
									
						
										
						- 
				JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Safety relating to thin fire kiln shelf paper
I almost always use "thinfire" (Papyros, actually) on non-slump firings and I never vent the kiln. It's been successful for me (so far! Jinx!!)Greg Rawls wrote:lmartine wrote:Your choice. I like to keep the smell contained.Greg Rawls wrote:Keep kiln closed when binders are burning off.
Dana W.
- 
				misteroldhouse
- Posts: 10
- Joined: Tue Dec 04, 2007 1:02 am
- Location: Dallas, Texas
- Contact:
Re: Safety relating to thin fire kiln shelf paper
Great question/great topic!
I would also add in my belief that a mask and gloves, even if latex-free, are not enough protection for any of us glass workers! I use those and vacuum the Thinfire off of the kiln shelf using a HEPA filtered long-handled vacuum.
When we brush that dust into a dust pan or whatever, some of the particles become airborne and remain so for a long time. I do similarly with me sandblaster, using a dust collected, mask & HEPA vacuum.
Larry Pile
			
			
									
						
										
						I would also add in my belief that a mask and gloves, even if latex-free, are not enough protection for any of us glass workers! I use those and vacuum the Thinfire off of the kiln shelf using a HEPA filtered long-handled vacuum.
When we brush that dust into a dust pan or whatever, some of the particles become airborne and remain so for a long time. I do similarly with me sandblaster, using a dust collected, mask & HEPA vacuum.
Larry Pile