I have a client of mines that wants me to make a trivet for her. I'm thinking that this kind of item will not be a smart idea because a trivet will have to withstand the placement of a very hot food item and I'm afraid that will be an easy case of thermal shock.
What do people think?
Thanks
Thanks
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Trivet
I think you are correct
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
Stephen Richard
- Posts: 302
- Joined: Sun Jul 06, 2003 4:36 pm
- Location: Glasgow, Scotland
- Contact:
Re: Trivet
I have a number in daily use.